Non Woven Fabric: Spunbond, Spunlace And GSM Cost
Home
Yiwu, Zhejiang, China
Mon – Fri 9:00 AM – 6:00 PM · Sat 9:00 AM – 4:00 PM
[email protected]

What Is Non Woven Fabric: The Web, The Bond And The Weight

Alan Xiao, Founder of Sourcing Pioneer
Alan Xiao Founder of Sourcing Pioneer
· Updated November 11, 2026 · 13 min read

A non woven fabric is a sheet of fibres held together by a bond, with no yarn and no weave in it.

The fibre goes down as a loose web first. Then heat, water, needles or a chemical binder locks the fibres to each other.

That is the whole idea, and it explains both the price and the failures. There is no spinning step and no loom, so the cloth is cheap per square metre. It is also weaker in the direction the fibres happen to lie.

This article gives the four routes that make the sheet. It also gives three checks that tell them apart on your desk. After that come the weight sums behind a bag quotation, and the one clause in European law that decides what you may call the material.

Studio still life of folded white non woven fabric sheets and a plain tote bag on a beige surface, soft daylight from the left
No yarn, no weave. The bond is the product.

The Short Answer

A nonwoven is an engineered sheet made straight from fibre or from molten polymer. The fibres are laid as a web, then bonded.

Industry bodies and standards define it the same way. The definition turns on how the sheet is held together, not on what it looks like.

Three things follow from that definition, and a buyer can use all three.

It is cheap because a step is missing. Woven cloth spins fibre into yarn, then weaves the yarn. A nonwoven skips both, so the cost is polymer, energy and line time.

Strength depends on the bond, not on the fibre. Two rolls from the same polymer can differ three times in tear strength. What changed is the bonding route and the weight.

Hand feel is a design choice. A stiff bag body and a soft wipe can come from the same machine family. The difference is fibre length and how the web was locked.

One warning before the detail. The word alone is not a specification. “Nonwoven” tells you there is no weave. It says nothing about the polymer, the route or the weight.

What The Word Actually Says

The name is a negative. It tells you what the sheet is not: not woven, not knitted, and in the standards, not paper either.

A workable description has two halves. First, how the web was formed. Second, how the web was bonded.

Web formation. Short fibres can be carded and crossed, laid in water, or blown in air. Long filaments can be spun and dropped straight onto a belt, with no cutting step at all.

Bonding. Calender rollers melt the fibres where they touch. Water jets tangle them. Barbed needles push them through the sheet. A binder glues them. Ultrasound welds them at points.

Put one word from each half together and the sheet becomes real. PP spunbond, thermal bonded, 60 GSM. PET needle-punched, 200 GSM.

Short fibres and long filaments are not the same trade. Wikipedia puts the staple lengths side by side. Wet-laid uses 0.64 to 1.91 cm fibres, air-laid uses 1.3 to 10.2 cm, and carding runs about 3.8 cm.

That difference shows up in the quote. Short fibres need opening, blending and a forming line. Filaments need a polymer feed and a die.

The lesson for an order is simple. Write the polymer, the route, the bond and the weight. Four words and a number beat one vague noun every time.

Four Routes, One Shelf

Most sourcing questions end on one of four routes. They are not grades of one product. They are different machines making different sheets.

Spunbond. Polymer is melted, pushed through a die, and the filaments are drawn and laid on a belt. The web is then bonded, usually by hot calender rollers. Filaments run about 15 to 35 micrometres across. The result is strong, stiff and cheap at volume.

Meltblown. The same polymer meets hot air at the die, so the stream breaks into very fine fibres, roughly 0.5 to 5 micrometres. The web bonds as it cools. It filters well and tears easily, so it is rarely used alone.

Spunlace. Short fibres are laid first, then hit with high-pressure water jets. The water tangles the fibres without melting or gluing them. The sheet drapes like cloth and blends viscose, cotton or polyester freely.

Needle-punched. A carded web runs under a board of barbed needles. The needles drag fibres down through the sheet thousands of times a minute. The result is thick and felt-like, and almost any fibre works.

The sandwich is the fifth item in the catalogue, and it is not a route. SMS means spunbond, meltblown, spunbond. Two strong skins carry a fine filter layer. SMMS and SSMMS add layers to shift the balance toward barrier or strength.

RouteFibreBondGood atCost
SpunbondContinuous filament, 15 to 35 µmHot calenderStrength, structure, bags and coversLowest
MeltblownMicrofibre, 0.5 to 5 µmSelf-bonded in hot airFiltration, barrierMiddle
SpunlaceShort staple, blendedWater jetsSoftness, absorbency, low lintHighest
Needle-punchedShort staple, any fibreBarbed needlesThickness, drainage, paddingMiddle
SMS sandwichSpunbond plus meltblownLayered, then bondedBarrier with strengthMiddle

Read the table down the cost column and one rule appears. Cost tracks the polymer and the energy, not the technology label. A spunlace wipe costs more than a spunbond bag because viscose costs more than PP, and because drying wet cloth burns fuel.

A supplier’s own comparison of the three routes ranks spunbond lowest and spunlace highest. It also notes that fibre choice and weight move the price more than the bonding method does.

Flat vector panel on a cream background comparing four nonwoven routes in four rows, each row naming the fibre form, the bonding step and the sheet it produces
Four routes, four bonds. The fibre is only half the answer.

Spunbond Or Spunlace: Three Checks On The Desk

Two samples can arrive in the same white envelope and feel nothing alike. Three checks settle which is which before you ask for a test report.

Hold it to the light. Spunbond shows a regular pattern of dots or diamonds. Those are the calender points where the rollers welded the sheet. Spunlace shows a random fibre surface, sometimes with a fine mesh from the water jets.

Drop water on it. A drop beads on untreated PP spunbond and runs off. It soaks into a viscose or cotton spunlace almost at once.

Tear it. Spunlace leaves a fuzzy, fibrous edge. Spunbond tears with a cleaner line and a small crackle, because the bond points break, not because the fibres pull out.

Feel completes the picture. Spunlace folds and drapes like a cloth napkin. Spunbond is crisp, springs back, and holds a crease badly.

These checks are not a lab result, and they should not be used to settle a dispute. They are there to catch the wrong roll before it reaches your line.

The commercial gap is large. Quoting a spunlace wipe as a spunbond wipe halves the material cost and fails the first wash. A factory that has both lines will quote the cheaper one unless the drawing says which.

The material also has a wet-strength problem worth naming. A spunlace sheet holds together in water because the fibres are tangled. A light spunbond wipe falls apart, which is why the two are never swapped in a wet product.

What GSM Settles, And What It Leaves Open

GSM means grams per square metre, and it is the first number on any nonwoven quotation. It is a weight, not a quality mark.

The measurement is simple and can be done at goods-in. Cut five discs of 100 square centimetres across the roll width, weigh each one, and multiply the average in grams by 100.

One supplier’s published notes on GSM set out the same method, with ISO 9073-1 and the EDANA procedure behind it. The five discs matter. A single disc can fall on a thin band and flatter the whole roll.

If you want the general arithmetic for cloth, a separate guide shows how fabric weight is read on a roll. This section keeps to what changes when the sheet has no weave.

The first thing GSM settles is what the sheet can be used for. Bag bands are well known in the trade.

GSMWhat it is used forWhat happens if you cut it
40 to 50Light retail bag, one or two itemsHandle pulls out, base seam splits
60 to 70Grocery bag, printed on one sideBase sags at the corners under load
80 to 90Heavy bag, box bag, laminated bagStiffer hand, higher freight per bag
100 and upReusable tote, promotional bagCost climbs faster than strength
Flat vector chart on a cream background with four weight bands from 40 to 100 grams per square metre, each band labelled with its bag use and the failure that appears when the weight is cut
Weight bands and the failure behind each one.

The second thing GSM settles is cash, through the tolerance band. This is the line most quotations leave out.

Suppose the order says 60 GSM. At a tolerance of plus or minus 2 GSM, the heaviest legal roll is 62 GSM. That is 3.3 percent more polymer than you asked for.

At plus or minus 5 GSM, the heaviest roll is 65 GSM, and the giveaway is 8.3 percent. On the light side the same band can deliver 55 GSM, which may fail your own load test.

Put the tolerance in writing, and ask for the weight to be reported on the delivery papers. A supplier who will not name a band is quoting plus or minus 5 or worse.

The third thing GSM does not settle is thickness. Bulk depends on how the fibres sit, not on how much they weigh.

Two rolls at 60 GSM can differ three times in caliper. A dense calendered spunbond is thin. A lofty needle-punched sheet of the same weight is thick.

So a drawing that asks for “60 GSM, 0.4 mm” is asking for two separate tests and two separate numbers. Neither one can be worked out from the other.

The Bag Sum: From GSM To Grams To Price

A bag quotation hides a small sum, and any buyer can run it. The weight of one bag is its area multiplied by the GSM.

Take a 40 by 46 centimetre bag with a gusset and two panels. Laid flat and opened out, that is roughly 0.4 square metres of cloth.

At 60 GSM, 0.4 square metres weighs about 24 grams. Ten thousand bags therefore eat about 240 kilograms of polymer before printing and waste.

Now add the loose tolerance. At 65 GSM the same bag weighs 26 grams, and the run needs 260 kilograms. That is twenty kilos you did not budget, on one order.

The same arithmetic checks a delivery. Roll weight in kilograms is GSM multiplied by width in metres, multiplied by length in metres, and divided by 1,000. A 50 GSM roll, 1.6 metres wide and 2,000 metres long, weighs 160 kilograms.

If the invoice says 2,000 metres and the scale says 150 kilograms, the roll is short or light. You can say which before you sign.

Number you needHow to get itWorked example
Area of one bagPanels opened out, in square metres0.4 m²
Weight of one bagArea × GSM0.4 × 60 = 24 g
Polymer for the runWeight × quantity ÷ 1,00024 × 10,000 = 240 kg
Weight of one rollGSM × width × length ÷ 1,00050 × 1.6 × 2,000 = 160 kg
Weight in ouncesGSM ÷ 33.90660 ÷ 33.906 = 1.77 oz/yd²

Then the part the sum does not explain. Twenty live listings for an 80 GSM printed bag, read on 11 November 2026, priced between 8 US cents and 60 US cents a piece.

Same weight, five times the spread. One listing offered a printed 80 GSM bag at 12 cents in a run of 1,000 pieces. Others sat at 18 to 30 cents at 3,000 pieces, and one asked 43 to 60 cents at 1,000.

Quantity is only part of it. Handle type moves the labour. A die-cut handle is punched in the same pass as the bag. A sewn handle is a separate operation and a separate needle. An ultrasonic handle needs a horn and a fixture.

Printing moves the cost twice, once for the plate and once for the colour count. Lamination adds a film and a gluing step. That is why a laminated bag at 80 GSM feels different from a plain one at the same weight.

This is the point to raise with the factory before samples. Ask for the bag weight in grams and the fabric GSM as two separate figures. A quotation that gives only one of them is not a specification yet.

How a bag plant sets up a line explains why the handle station, not the fabric, often sets the smallest order a factory will take.

The Four Numbers On A Datasheet

A nonwoven datasheet usually carries four numbers. Each one belongs to a named method, and the method number is what makes the figure checkable.

Weight. ISO 9073-1 covers mass per unit area. It is the GSM line, and it is the only one your own scale can confirm.

Thickness. ISO 9073-2 measures caliper under a set pressure. Without the pressure stated, the figure means little, because a soft sheet compresses.

Tensile strength. ISO 9073-3 pulls a strip until it breaks. Nonwoven is not the same in both directions, so the report has to say machine direction or cross direction.

Barrier. A hydrostatic head test, ISO 811, holds a column of water against the sheet and records the height at which it passes through. For masks and gowns, a bacterial filtration test such as ASTM F2101 is quoted as well.

Two trade bodies keep the same methods in a second numbering. INDA and EDANA publish the Nonwovens Standard Procedures that both bodies maintain. The set was first issued in 2005 and is revised as methods change. Many of those procedures are also adopted by ISO or CEN. A datasheet may cite either number.

Ask which body the number comes from, and ask for the report page, not the summary line. A figure copied from a similar product is common, and it is invisible until a claim is tested.

The same logic applies at goods-in. What an inspector checks on a fabric roll is a weight and a width, measured in three places. The roll edge is checked for crush damage as well.

What The Law Calls This Material

Europe wrote a definition that decides what you may call a nonwoven product. It turns on the polymer, not on the process.

Directive (EU) 2019/904 defines plastic as a material made of a polymer. Additives are allowed, and the material has to act as the main structural part of a product. One exception is written into that sentence: natural polymers that have not been chemically modified.

That exception is doing a lot of work. A PP spunbond bag is plastic under that test. A viscose sheet is the hard case, because the cellulose started natural and was changed on the way to fibre.

The Directive’s own text is short enough to read in a sitting. The text of Directive (EU) 2019/904 is the version to quote, not a summary from a supplier.

Now the part most buyers get wrong. Wet wipes were not banned.

The ban list in Part B covers cotton bud sticks, cutlery, plates, straws, stirrers, balloon sticks, and food or drink containers made of expanded polystyrene. Wipes are not on it.

Wipes are in Part D instead, which is a marking duty. Since 3 July 2021, a pre-wetted personal care or domestic wipe has to carry a marking on the sales packaging and on grouped packaging. Packaging smaller than 10 square centimetres is excused.

The same product sits under extended producer responsibility, so the importer carries a cost for the waste it creates.

Three practical lines follow. First, the importer is the one who answers for the label, not the factory. Second, the artwork is a legal document and should be signed off before plates are cut. Third, the material definition is separate from the marking rule, so a “paper” wipe is not automatically outside the Directive.

Nothing in the Directive bans nonwoven bags made of PP. They are a plastic product, and the bag rules come from a different directive on packaging and carrier bags.

Three Claims That Fail After The Boat Leaves

A claim is cheap to print and expensive to defend. Three turn up on almost every nonwoven product, and each one has a check you can run.

“Biodegradable”. This word has no agreed test behind it for a nonwoven sheet. The Directive also treats oxo-degradable plastic as a problem material in its own right. Ask for the test method and the conditions, in writing. If the answer is a logo, the claim is not supported.

“Eco friendly”. Nothing measures it. A bag made of a thinner sheet uses less polymer, and that is a real gain. A bag that tears on the second trip is not a gain. Replace the phrase with a number: bag weight, recycled content, number of trips in a load test.

“Reusable”. A reuse claim needs a load test and a trip count. A 50 GSM bag and a 100 GSM bag look similar in a photo and behave differently in a trolley. Your own load test is the only evidence that travels with the goods.

The fibre content is the fourth item to pin down, because it is printed on the label in some markets. Write the blend as percentages on the order, and keep a sample of the roll that the label describes.

What a biodegradable claim has to survive is worth reading before the artwork stage, not after it. The importer carries the cost of a wrong word.

One more check belongs here. A nonwoven sheet is often laminated to a film to carry a print or hold liquid. The laminate is a second material with a second set of rules, and it is the part that usually breaks a recycling claim. The other materials on the same shelf lay out how film, paper and cloth compare.

Six Lines For The Order Sheet

A nonwoven order fails in the same six places every time. Each line below closes one of them, and each fits on an order sheet.

  1. Polymer and route. PP spunbond, PET needle-punched, viscose and PET spunlace. Name the fibre and the process, not just the word nonwoven.
  2. Bond. Calender bonded, water jet, needle-punched, or a named sandwich such as SMS. The bond sets the hand feel and the tear strength.
  3. Weight and band. Write 60 GSM plus or minus 2, and say where the five discs are cut across the roll width.
  4. Width and roll form. Width in millimetres, core diameter, roll length, and the winding direction if the converting line needs one.
  5. Test numbers. Name ISO 9073-1, 9073-2 and 9073-3, or the matching NWSP number, and ask for the report page with the shipment.
  6. Label and claim. The fibre blend in percentages, the marking artwork where the law asks for one, and the load test for a reuse claim.
Flat vector checklist on a cream background with six numbered lines for a nonwoven order, each followed by the short example value a buyer should write
Six lines, one page, no argument later.

The order also needs a reference sample that both sides signed. A photo will not do, because a second roll can be a shade darker and still be correct.

Keep the sample with the paperwork. When a second order arrives lighter than the first, the argument is settled by a scale and a signed bag, not by memory.

Finally, write the tolerance into the price, not into the chat. A supplier may agree plus or minus 2 GSM in an email, then quote plus or minus 5 on the invoice. That is two different products. The spec sheet the plant works from is the document that decides which number the line follows.

WEIGHT CHECK

Send me a nonwoven quotation and the sample weight behind it. I will check the polymer, the route, the GSM band, and the bag sum against the finished bag weight. Then I will tell you which line is missing, before you pay a deposit or cut a plate.

Check The Weight

Questions Buyers Ask

Is non woven fabric plastic?

It depends on the polymer. A PP or PET sheet is plastic under the EU definition. A viscose sheet is the arguable case, because the cellulose was chemically changed on its way to fibre.

Can non woven fabric be washed and used again?

Some can. A 90 GSM spunbond bag survives many trips, while a 40 GSM one is a single-use bag with a handle. A reuse claim needs a load test, not a photograph.

Which GSM should a shopping bag be?

Forty to 50 GSM suits light retail, 60 to 70 covers grocery weight, and 80 to 90 is the heavy and box bag range. Test the lightest candidate instead of defaulting to the heaviest.

Spunbond or spunlace, which is stronger?

Spunbond, at the same weight. Continuous filaments resist tearing. Spunlace wins on softness and absorbency, which is why wipes use it and bags do not.

Why is my 60 GSM roll lighter than the sample?

A tolerance band allows it. At plus or minus 5 GSM a 60 GSM order can arrive at 55 GSM. Weigh five discs across the width and compare with the signed sample.

Does a heavier sheet always last longer?

Not on its own. Bonding and fibre length matter as much. A well bonded 60 GSM sheet can outlast a badly bonded 80 GSM one in the same load test.

Questions & Comments

We read every one and reply within 24 hours

If a nonwoven quotation lands on your desk, send it over with the bag weight in grams. I will check the route, the GSM band and the polymer, and say which line the plant will read differently.

Subscribe
Notify of
guest
0 Comments
Most Voted
Newest Oldest
0
Would love your thoughts, please comment.x
()
x