What Is Anodizing: An Oxide Grown From the Metal
Anodizing is an electrical bath that makes the oxide layer on a metal part grow thick. The part is the positive electrode. Oxygen forms on its surface, and the oxide builds outward and inward at once. Nothing is painted on, so there is no layer to peel off. The colour, when there is one, goes into pores in that oxide afterwards.
That single mechanism explains most of what buyers get wrong about the process.
It is why an anodized part can be scratched without exposing bare metal underneath. It is also why the same part grows on every face. Anyone holding a drawing with tight tolerances finds that out the hard way.
This page covers how the layer grows and what Type I, II and III mean in microns. Then how the colour goes in, where the finish fails, and what to write on a drawing.
The Short Answer
The anodizing process thickens the natural oxide that air already puts on aluminium. Bare aluminium forms a layer 2 to 3 nanometres thick on its own. The bath takes that to a few microns or more.
The layer is harder than the metal and it does not conduct electricity. It resists corrosion because it seals the surface away from air and water. It holds dye because of how it grows.
It is also not a coating in the usual sense. Paint and plating sit on top of a surface. They can lift or flake from an edge. An anodic layer is converted metal, so it can crack under stress but it cannot peel.
Aluminium is the common case, and the rest of this page stays with it. The same idea works on titanium, zinc, magnesium, niobium, zirconium and tantalum. Each metal needs its own bath.
How the Layer Grows
The part hangs on a rack in an acid bath and carries a direct current as the positive electrode. Oxygen forms at its surface and combines with the metal into oxide.
The acid does two jobs at once. It grows the oxide and it slowly dissolves it. The balance between those two rates is what makes the layer porous rather than dense.
The pores are the point. They run from 10 to 150 nanometres across and let the bath reach the metal underneath. That is how the layer grows far past what air alone would ever produce.
The same pores take up dye afterwards. That is why a colour sits inside the finish rather than on it. A scratched part still shows colour in the scratch.
The bath is usually sulfuric acid. Chromic acid came first, in 1923, on seaplane parts. It is still used where its properties are needed. Sulfuric acid was patented in 1927 and remains the common choice.
Voltage mostly sits between 15 and 21 volts. Across all processes the range runs from 1 to 300. Current scales with the area of the part, typically 30 to 300 amperes per square metre.
The thickness range across the trade runs from under half a micrometre to about 150. The thin end keeps a polished surface looking bright. The layer there is too thin to dull it. The thick end belongs to window frames and roof sections. There the layer has to survive weather for decades.
Thicker and harder layers come from a more concentrated bath. It runs colder, with more voltage and current. A hard-coat bath runs near the freezing point of water. That is why it costs more to operate.
Three Types, and What the Numbers Mean
The trade names come from a United States military specification. It is called MIL-PRF-8625. It defines three types. The type is really a statement about the bath and the thickness.
| Type | Bath | Thickness | Where it is used |
|---|---|---|---|
| I | Chromic acid | 0.5 to 18 µm | Aerospace, paint pretreatment, thin protective work |
| IB and IIB | Chromic and sulfuric | Thin, similar to Type I | Parts where a thick layer would change the fit |
| II | Sulfuric acid | 1.8 to 25 µm | General purpose, dyed cosmetic parts |
| III | Sulfuric, refrigerated | Over 25 µm, up to about 150 | Wear surfaces, hard coat, engineered parts |
| IC | Organic acid | Up to 50 µm | Colour from the bath, no dye |
Two things about that table catch buyers out. The first is that Type II and Type III use the same acid. Thickness and process control are the difference. The second is that the specification does not tell a factory how to run the bath.
These documents define the tests and the quality checks a finished part must pass. They do not define chemistry. A drawing that cites a specification is describing an outcome, not a recipe.
Sometimes a thin layer is all the fit allows. The Type IIB route exists for exactly that case, where a thick coat would break tolerance. That is a fit question before it is a finish question.
It Changes the Size of the Part
This is the most expensive misunderstanding in the whole process, and it is arithmetic.
The oxide grows down into the metal and out from it by equal amounts. So each coated face moves outward by half the coating thickness. The old surface ends up in the middle of the layer.
A 2 micrometre coating therefore grows every face by 1 micrometre. If the part is coated on all sides, every linear dimension grows by the full coating thickness.
On a 20 micrometre cosmetic layer, a 10 mm shaft becomes 10.02 mm. That is enough to fail a bore, a thread or a press fit machined to the drawing size.
There are two normal answers. Machine the part undersize by the coating allowance, or mask the surfaces that must stay bare. Both belong on the drawing, and neither can be decided by the factory alone.
Where the Colour Comes From
Three different mechanisms produce anodized colour, and they behave differently in production.
The common one is dye. After anodizing, the part goes into a dye bath and the pores take up colour. A seal then closes them. The usual seal is nickel acetate, and without it the dye does not stay.
The dye only occupies the outer part of the layer, so a scratch may show a lighter shade. The oxide underneath keeps protecting the metal even where the colour is gone.
The second mechanism puts the colour in during the bath itself, using organic acids. It gives pale yellow, gold, deep bronze, brown, grey and black. It also does not fade the way dye can.
It also has a production problem that buyers should know about. The shade is sensitive to the alloy underneath. The reference literature describes it as impossible to repeat reliably.
The third mechanism is not aluminium at all. On titanium, colour comes from thin-film interference. The same bath at different voltages gives different hues, with no dye involved.
What It Cannot Do
Several limits belong in the conversation before a sample is approved.
Anodizing does not make a part stronger. It changes the surface, not the bulk metal, so a weak alloy stays weak.
The layer is brittle in a particular way. It has lower thermal expansion than the metal beneath. So it will crack under thermal stress above roughly 80 degrees Celsius. It cracks; it does not peel.
It is also sensitive to chemistry at both ends of the pH scale. A strong acid or a strong alkali will dissolve the layer and expose the metal. That is why a coated part does not suit a cleaning regime built on caustic wash.
Two process faults show up as appearance defects. Too much current or voltage causes burning, where large uneven black regions form. Some organic acids can run away and pit the surface badly.
| What you see | Usual cause | What it tells you |
|---|---|---|
| Uneven black patches | Burning, from too much current or voltage | The bath is not being controlled |
| Pits or scars | Runaway attack in an organic acid bath | The wrong bath for that alloy |
| Patchy or dark tone | Copper or silicon in the alloy | The metal is fighting the finish |
| Colour rubbing off | Dye with no seal, or a poor seal | A step was skipped after anodizing |
| Fine cracks after use | Thermal stress above about 80 degrees | Normal for a thick layer, not a fault |
Finally, the layer is an electric insulator. That is useful on a housing and awkward on a part that must be earthed. There, a masked contact area or a chromate conversion coat on that patch does the job.
The Alloy Decides the Finish
Two parts can go through the same bath on the same day and come out looking different. The variable is usually the metal, not the process.
The process works on aluminium alloys, and the alloying elements matter. Copper, iron and silicon are named in the reference literature as the elements that cut its corrosion resistance.
The 2000, 4000, 6000 and 7000 series are described as the most susceptible for that reason. That does not rule them out. It does mean the alloy comes before any finish is promised.
A high-silicon casting grade is a poor candidate for a cosmetic layer. The elements that make it easy to cast spoil a uniform finish.
There is a standard for this choice, BS 1615, which guides alloy selection for anodizing. The short version is simpler. Put the alloy and temper on the drawing, and let the finisher quote against that metal.
Where the choice is still open, the alloy choice for the part changes both the finish and the price.
Seven Lines for the Drawing
A drawing that says “anodized black” is an instruction to guess. These seven lines remove the guesses.
- Alloy and temper. Name them, and say which faces are cosmetic. A finisher quotes differently once it knows which surfaces must be perfect.
- Type and thickness. Write the type and a thickness range in micrometres, for example Type II at 15 to 20. A single number with no range is hard to hold.
- Colour and reference. Give a physical sample or a colour reference, and state whether the colour is a dye or comes from the bath. Add the light-fastness expected.
- Seal. Name the seal for any dyed part, and say that it is required. Unsealed dye comes off on a thumb.
- Masking. List the surfaces that stay bare: threads, bores, mating faces and earth contacts. This is the line that prevents a fit failure.
- Dimensional allowance. Say whether the part is machined undersize or the growth is accepted, and by how much per surface.
- Rack marks and test. Say where contact points may fall, and name the checks: coating thickness, seal quality, colour against the approved sample.
Line six is the one that saves a shipment. Half the coating goes into the metal and half comes out of it, so every face moves. A supplier who is not told about the allowance will not invent one.
That decision is made at the machine, not the bath. Machining the part before finishing sets the tolerance the finisher has to live with.
None of this fits on a single line of an order. The drawing that goes with the order is where those seven lines become enforceable. It is also where a factory can be held to a number rather than an impression.
How to Compare Two Quotes
Three checks separate a real quote from a plausible one.
First, look for the type and a thickness range. A quote that says “anodized” without either leaves the costliest variable open. Type III at 50 microns is a different job from Type II at 15.
Second, ask which alloy the price assumes. A quote built on a free-machining grade will not survive a change to a cosmetic one. The price should move when the metal moves.
Third, ask who masks the part and who inspects it. Masking is labour, and it is the step most often quietly dropped when a price is squeezed.
After those three, price and lead time belong in the conversation. A finish that fails the first container costs more than the difference between two quotes.
Where the claim finally gets tested is the paperwork that ships with the parts. The coating test report settles an argument about a colour agreed in a message.
Half the Coating Grows Into the Part
Send me the alloy, the fit that must be held and the finish you want on the drawing. I will tell you the allowance to machine and which surfaces to mask. I will also say what to write so the first container matches the sample. That costs nothing before tooling.
Send the DrawingIs anodizing the same as powder coating?
No. Anodizing converts the surface metal into oxide, so there is no applied layer to peel. Powder coating sprays a plastic film on top and cures it, and can be removed again.
Does anodizing stop corrosion completely?
No. The layer resists corrosion well when it is sealed, but microscopic fissures can still let corrosion start. Strong acids and strong alkalis dissolve the layer and expose the metal.
Why did my part not fit after anodizing?
Because the layer grows outward as well as inward. Each coated face moves by half the coating thickness. A 20 micron layer therefore adds 0.02 mm to a dimension.
Can anodized aluminium be welded afterwards?
It is harder. The oxide is an electrical insulator and melts at around 2,050 degrees Celsius, against 658 for the aluminium. Most work is welded first and anodized afterwards.
Can I have any colour?
Dye gives a wide range, and it can fade under sunlight. Colour from the bath is limited to yellows, bronze, brown, grey and black. On titanium, colour comes from film thickness rather than dye.
Is hard anodizing always better?
No. Type III resists wear better, but it is more brittle and changes the part size more. For a cosmetic housing, Type II at 15 to 20 micrometres is usually the right finish.
Questions & Comments
We read every one and reply within 24 hoursHalf the coating grows into the part and half comes out of it. Tell me the fit you must hold and the finish you want, and I will say what to machine and what to mask.