What Is Powder Coating: A Plastic Film, Baked On
Powder coating sprays a dry plastic powder onto a part and charges it so it sticks. The part is then baked until the powder melts into a film. Nothing evaporates away, so the coat can be thick without running. It is an applied layer, not a change to the metal. That is the one thing that separates it from anodizing.
That difference decides most of the arguments buyers have with factories.
An applied film can chip at an edge and lift from a scratch. A converted oxide layer cannot peel. Both are sold as “a finish”, and they fail in opposite ways.
This page covers the three steps and the powder types. Then why thin coats are hard, the corner that never gets covered, and what to write on a drawing.
The Short Answer
Powder coating is a finishing process. A dry powder is sprayed onto a grounded metal part. Static charge holds it there.
The part then goes into an oven. The powder melts and flows into an even film. It cures into a hard layer as it cools.
Two families of powder exist. A thermoset powder reacts chemically and cannot be re-melted afterwards. A thermoplastic powder simply melts and flows, with no reaction.
The process was invented around 1945 and patented the same year. It was used first on household appliances, aluminium extrusions and bicycle frames. It still is.
There is no liquid carrier, so the coat can be built thick. It does not run or sag the way a wet paint does. It also gives off very few solvents, which is why the process spread.
Powder, Charge, Oven: Three Steps
Every powder line does the same three things, whatever the part is.
The first step is preparation. Oil, dirt, grease, metal oxide and welding scale all have to come off. Nothing sticks until they do.
Chemical prep runs the part through several stages. Degreasing comes first, then etching, a de-smut rinse, and a phosphate or chromate coat that gives the powder a grip.
Chromate has been losing ground for environmental reasons. Titanium, zirconium and silane treatments now do the same job on many parts.
Mechanical prep is blasting: grit, glass bead, plastic media or steel shot. It removes scale and leaves a texture the powder can key into.
The second step is application. A spray gun gives the powder a negative charge. The grounded part pulls it in. The coating builds until the charged layer starts to repel new particles.
Some lines preheat the part before spraying. That gives a more even film but risks runs where too much powder lands.
The third step is curing. The part sits in an oven until the powder melts and, for a thermoset, cross-links. Common schedules are 200 degrees for 10 minutes, or 180 for 10 to 15.
European and Asian lines have run 180 degrees for decades. Many are moving to 160 to save energy. Indoor hybrid powders can cure near 125 to 130.
Three Families of Powder
The powder is not one material. The three families below behave differently in the oven and outdoors.
| Family | How it sets | Typical use | What to watch |
|---|---|---|---|
| Thermoset, hybrid | Polyester and epoxy react together | Indoor parts: shelving, cabinets, furniture | Poor outdoor colour hold |
| Thermoset, TGIC | Polyester with a TGIC hardener | Outdoor: frames, garden furniture, poles | Hardener is under regulatory pressure |
| Thermoset, HAA | Polyester with a TGIC-free hardener | Outdoor, where TGIC is restricted | Tends to yellow if overbaked |
| Polyurethane | Hydroxyl resin plus blocked isocyanate | Thin, smooth and durable films | Needs a higher deblocking temperature |
| Thermoplastic | Melts and flows, no reaction | Thick protective coats, racks, pipe | Softer, and re-melts with heat |
| UV-curable | Melts, then cures under ultraviolet light | Heat-sensitive board and composites | Line of sight is needed for the light |
Two numbers explain the mixing ratios you will see on a datasheet. Hybrid powders are sold as 50/50, 60/40 or 70/30. That is the polyester-to-epoxy share. Outdoor TGIC powders run at about 93/7.
UV powder is the odd one out on time. It melts in 60 to 120 seconds at 110 to 130 degrees, and cures the moment the light hits it. That is why it is used on medium-density board and composites. Neither can survive a normal bake.
The chemistry also carries small helpers. A flow promoter lets the melted film level out. Benzoin is added to degas it, so the film does not end up full of pinholes.
Why Thick Is Easy and Thin Is Hard
This is the counter-intuitive part of the process. It catches buyers who ask for a thin coat to save money.
Powder grains run from 2 to 50 microns. They soften near 80 degrees, melt near 150, and flow together in the oven.
Coarse grains do not pack into a thin even layer. As the film gets thinner, the surface turns into what the trade calls orange peel. It looks like the skin of the fruit.
In practice a film build above 50 microns is needed for an acceptably smooth finish. Below that, the texture is a property of the powder rather than the operator.
There are exceptions. Some lines run powders under 30 microns, or with a much lower softening point, to get a smooth thin film. A slurry process grinds powder to 1 to 5 microns and disperses it in water for the same reason.
One more point that surprises buyers. Many finishers prefer some orange peel on purpose. A slightly textured surface hides dents in the metal. It also shows fingerprints far less than a mirror-smooth film.
The Corner That Never Gets Covered
A recessed area is the hardest place to coat, and the reason is physics rather than skill.
A charged grain flying toward a grounded part is pulled to the nearest earthed surface. The walls of a deep channel screen the field, so the inside of the channel sees very little of it.
The effect has a name, the Faraday cage, and it starves recesses of powder. The outer face builds a full film while the inside of the channel stays thin.
A corona gun makes it worse. It can also reverse the charge on a layer that is already thick. That fault is called back-ionization. It shows up as pinholes and a rough patch.
There are two answers. A tribo gun charges the powder by friction against a tube, not by a high-voltage field. It is described as free of both problems.
The other answer is a fluidized bed. The part is heated and dipped into aerated powder. Powder coats every surface it touches. That route is used when the coat must exceed 300 microns. Dishwasher racks are the classic case.
For a buyer, the practical test is simple. If the drawing has a deep pocket, a narrow slot or an internal corner, ask which gun will reach it. Then ask what thickness is guaranteed inside.
What It Cannot Do
Four limits belong in the discussion before a sample is approved.
The part has to be able to hold a charge, which in practice means metal. Powders for plastic, composite, glass and wood exist, but they need extra surface treatment or a UV cure line.
The part also has to fit in an oven. That single fact decides whether a large welded frame is powder coated or wet painted.
The cure temperature rules out anything that cannot take 160 to 200 degrees. Low-temperature powders help, but the reference literature notes they hold colour less well than a standard bake.
Removal is the fourth limit. There is no solvent that simply washes the film off. Methylene chloride and acetone work, and most other solvents do nothing. The industrial routes are abrasive blasting, or a burn-off oven at 300 to 450 degrees for about four hours.
| What you see | Usual cause | What it tells you |
|---|---|---|
| Dimpled surface | Film too thin for the powder grade | The build is under about 50 microns |
| Pinholes | Gas escaping, or back-ionization | Degassing additive missing, or too much voltage |
| Thin patch inside a recess | Faraday cage effect | The wrong gun for that shape |
| Peeling from an edge | Preparation was skipped | The film never bonded to the metal |
| Yellowing after the oven | Overbake on a low-temperature powder | Oven time or temperature drifted |
Coating or Conversion
Powder coating and anodizing are often quoted against each other for the same aluminium part. They are not variations of one process.
Anodizing converts the surface metal into oxide. Half the layer grows into the part and half comes out of it. Nothing can peel, because nothing was added.
Powder coating puts a plastic film over the surface. It is thicker, usually 60 to 100 microns against 15 to 20 for a cosmetic anodic layer. It also hides machining marks that anodizing would show.
The failure modes run in opposite directions. A converted layer cracks under thermal stress but stays on. An applied film resists cracking and can lift from an edge where the bond was poor.
Substrate is the other deciding factor. Anodizing is an aluminium process. Powder coating works on steel and aluminium alike. That is why welded frames and sheet metal almost always go this way.
Colour range also differs. Powder reaches most of the colour space and gives gloss control. Anodizing dyes are wide but the finish is translucent, and the metal shows through.
If the part is aluminium and the priority is wear resistance without a film, the conversion route wins. That comparison is set out in the anodizing explainer. If the part is steel, or the priority is colour and hiding, this route wins.
Seven Lines for the Drawing
“Powder coated black” is not a specification. These seven lines make it one.
- Substrate and preparation. Name the metal, and name the pretreatment: phosphate, or a chrome-free titanium, zirconium or silane route.
- Powder family. Say whether the part is indoors or outdoors, and name the family. A hybrid powder outdoors is a warranty problem waiting to happen.
- Colour and gloss. Give a colour reference such as an RAL number, and add a gloss level in units. “Matte black” covers a wide range.
- Film thickness. Give a target and a minimum, for example 70 to 90 microns, and state the minimum inside recesses separately.
- Coverage of recesses. Name any pocket or slot, and say what thickness must be reached inside it. This is where the Faraday cage bites.
- Cure schedule. Write the temperature at the part and the time, not the oven setting. A heavy part takes longer to reach temperature than a thin one.
- Tests. Name the checks: film thickness, adhesion by cross-hatch, impact, colour against the approved sample. Add salt spray if the part lives outdoors.
Line five is the one nobody writes and everybody argues about later. A recess that measures 30 microns when the flat face measures 80 is not defective by the letter of most drawings. The drawing never said.
The thin-gauge side of the same problem belongs to the fabricator. A part with thin walls warps in the oven, and stamping and machining the part sets the wall thickness the coater has to work with.
All seven lines end up in one document. The spec sheet factories work from is where a finish becomes enforceable rather than a matter of opinion.
How to Compare Two Quotes
Three checks separate a real quote from a plausible one.
First, look for the powder family. A quote that names no family cannot be compared, because an indoor hybrid and an outdoor polyester differ in price and in life.
Second, ask what pretreatment the price includes. Degreasing alone is cheaper than a full phosphate line, and it is the step that decides whether the film stays on.
Third, ask for the film thickness range and the cure schedule. A coater that cannot state either is running by feel.
After those three, price and lead time come later. A film that fails adhesion in the first year costs more than the gap between two quotes.
Where the claim is finally tested is the paperwork that ships with the parts. The test report for a finished part is what settles an argument about a colour or a thickness agreed in a message.
The Inside of a Pocket Coats Thinner
Send me the part drawing, the metal and where it will be used. I will tell you which powder family the job needs and what thickness to demand inside a recess. I will also say where the drawing is silent in a costly way. That costs nothing before tooling.
Send the DrawingIs powder coating better than paint?
It is thicker and tougher, and it releases far fewer solvents. Wet paint still wins where the part cannot take oven heat. It also wins where a very thin film is needed, or where a finish must be touched up on site.
Can powder coating be used on aluminium?
Yes, and aluminium extrusions are one of its oldest uses. The choice against anodizing is a choice between an applied film and a converted oxide layer, not between good and bad.
Why does my part have orange peel?
Usually because the film is thinner than the powder grade can flow out. Particles of 2 to 50 microns need roughly 50 microns of build to level into a smooth surface.
Can a chip be touched up?
Not the way paint can. A cured powder film is cross-linked, so a repair means stripping and recoating the part. The other choice is a touch-up pen that will not match the texture.
Does powder coating conduct electricity?
No. The film is an insulator, so any earth contact or conductive path has to be masked before coating and left bare afterwards.
Which powder lasts outdoors?
An outdoor polyester, either TGIC-cured or the TGIC-free HAA type. Hybrid powders that mix polyester with epoxy are for indoor use, and their colour will not hold outside.
Questions & Comments
We read every one and reply within 24 hoursA deep pocket coats thinner than a flat face, and most drawings never say so. Tell me the part and where it lives, and I will say which powder and what thickness to demand.