What Is TPR Material: A Rubber That Melts
TPR material is a rubber-like compound that melts when heated, so it runs on the same machines as plastic.
TPR stands for thermoplastic rubber. The name carries the whole idea: it feels like rubber and it processes like plastic.
That one property decides where it belongs. A soft grip on a can opener and the skin of a yoga mat are often the same family of material.
This article covers what the name means, what a datasheet prints and how the soft part bonds to the hard part. It ends with the six lines an order needs.
The One-Sentence Answer
TPR is a plastic you can stretch. Heat it and the chains slide, so it flows into a mould. Cool it and the rubber behaviour comes back.
Nothing is cured. No chemical reaction locks the shape, which is the opposite of a tyre or a silicone spatula.
A silicone part is a thermoset. Once it sets it cannot be melted again, and a bad shot stays scrap.
A TPR part can be melted again. The runner, the sprue and the reject can go back into the machine, and that is why the material suits long moulding runs.
The formal wording is short. The body that names polymers calls this class an elastomer with a network that breaks on heat and re-forms on cooling.
In a quotation nobody says elastomer. Buyers say TPR, TPE or soft-touch compound, and most of the time the three words point at the same pallet of pellets.
Why One Name Covers Several Rubbers
Six material classes sit under the thermoplastic elastomer name. The standard that names them, ISO 18064, gives each one a short code.
They are TPS for styrene block copolymers, TPO for olefin blends, TPV for vulcanised blends, TPU for polyurethane, TPC for copolyester and TPA for polyamide. A seventh code, TPZ, catches the unclassified ones.
The first class is what most people mean by TPR. A TPS chain has a hard styrene end, a soft rubber middle and another hard end.
At room temperature the ends clump together and act as the cross-links. Heat melts the clumps, and that is the whole trick.
Two versions of that chain matter to a buyer. SBS keeps double bonds in the rubber middle. SEBS is the same chain after hydrogenation, so those bonds are gone.
The difference is not academic. The double bonds react with oil, oxygen and sunlight, so an SBS grip goes tacky while an SEBS grip holds its feel.
Most grips, mats and toy parts are a compound, not a pure polymer. The block copolymer is mixed with mineral oil for softness, polypropylene for strength and filler for cost.
That is why two samples sold as “TPR 60 Shore A” can behave like different materials. The label names a family, and the recipe decides the rest.
The same loose naming shows up in other product groups. A toy programme will quote TPR next to PU and silicone under a single price list, and the three feel nothing alike in the hand.
The Numbers On A TPR Datasheet
Ask for a datasheet before you ask for a price. A real one prints the same lines, and those lines answer most of the questions a buyer has.
The figures below come from one published series, the AD1/CS range from KRAIBURG TPE. They are typical values for that range, not an average of the market.
| Spec line | What this series prints | Why a buyer cares |
|---|---|---|
| Hardness | 47 to 80 Shore A | How soft the grip feels |
| Density | 1.100 g/cm³ | Weight per part and freight per carton |
| Tensile strength | 3.5 to 10.0 MPa | Pull before the part tears |
| Elongation at break | 500 to 600 % | Stretch before failure |
| Tear resistance | 11.0 to 24.5 N/mm | How a nick spreads |
| Peel adhesion to ABS | 3.0 to 6.0 N/mm | Whether the grip stays on |
| Peel adhesion to PC | 2.0 to 10.0 N/mm | The same bond on another plastic |
| Compression set, 24 h at 100 °C | 60 to 76 % | Recovery after a clamp |
| Mould temperature | 40 to 60 °C | Cycle time and clean release |
Start with density, because it is the line that reaches the freight invoice. At 1.100 g/cm³ a grip is not a light part, and the carton weight follows the shot weight.
Hardness sets the feel and the price. A 47 Shore A grip is soft enough for a jar opener, and an 80 Shore A compound is closer to a shoe sole.
Then read the two adhesion lines together. The same compound reaches 3.0 N/mm on ABS and 10.0 N/mm on PC, so the substrate decides the result as much as the grade does.
The compression set line is the one buyers skip. At 100 °C the series recovers to only 60 to 76 %. That explains why a TPR foot flattens under a heavy board.
None of these numbers survives a bad process. A grade that prints 10.0 N/mm will still peel if the tool runs cold or the gate sits in the wrong place.
How A Soft Grip Bonds To A Hard Handle
Most TPR in a kitchen is a second shot over a hard plastic. The handle is polypropylene or ABS, and the grip is moulded straight onto it.
The bond is part mechanical and part chemical. The melt wets the hard surface, and the two materials lock together as the part cools.
Peel strength is the number that describes that bond, in newtons per millimetre of width. The series above prints 3.0 to 6.0 N/mm on ABS.
A grip at 5 N/mm survives a drawer full of tools. A grip at 1 N/mm comes off in a wash cycle, and the buyer reads about it in a review.
Three process points decide whether the part reaches the datasheet figure or misses it.
Mould temperature comes first. The hard part has to be warm when the soft shot arrives, and the datasheet asks for 40 to 60 °C.
The ceiling matters as much as the floor. Above 80 °C the compound can degrade in the barrel, so the tool needs its own temperature control.
Gate position comes second. The melt has to reach the bond line while it is still hot, or it freezes before it touches the surface.
Wall thickness comes third. A very thin skin cools in a fraction of a second, so most grips are moulded thicker than a decorative cap.
Drying is the step that gets skipped when the workshop is busy. The datasheet asks for two to four hours at 60 to 80 °C before the pellets go into the hopper.
Wet pellets do not stop the machine. They leave a dull surface, a weak weld line and a bond that fails later, which is the worst kind of fault.
One design note sits above all of it. A small mechanical key, a groove or a through-hole gives the soft shot something to hold, so the grip is not standing on adhesion alone.
TPR, TPE And Silicone Side By Side
This is the part buyers read twice, because all three names turn up in one quotation and the prices differ by a wide margin.
TPE is the family name and TPR is one branch of it. Silicone is not in the family at all, because it cures instead of melting.
| Question | TPR (TPS type) | Silicone | TPU |
|---|---|---|---|
| What it is | Styrene block copolymer compound | Cured silicone rubber | Polyurethane elastomer |
| Melts again | Yes | No | Yes |
| Feel at the same hardness | Soft, slightly waxy | Silky and dry | Firmer, more plastic |
| Heat ceiling | 60 to 80 °C, near 100 °C in special grades | Far higher, above 150 °C in reported use | About 100 to 120 °C |
| Oil and grease | Poor on SBS, better on SEBS | Fair | Good |
| Sunlight | Poor unless stabilised | Good | Poor on standard grades |
| Bond to polypropylene | Designed for it | Needs a primer or a mechanical grip | Limited |
| Scrap | Can be melted again | Cannot | Can be melted again |
| Cost direction | Lowest | Highest | Middle to high |
The heat line is the one that settles most arguments. A TPR part that meets a hot pan softens, and a silicone part keeps its shape.
The heat figures are reported, not fixed by a standard. An engineering guide puts general TPR at 60 to 80 °C, and a moulder’s guide gives −50 to 80 °C for the same class.
The bond line settles the rest. TPR is made to stick to polypropylene in the tool, and silicone needs a primer or a mechanical hold.
Cost follows the chemistry. TPR is the cheap option, silicone is the costly one, and a supplier who quotes silicone at a TPR price is quoting something else.
TPU sits between them. It wins on oil, wear and tear, and it loses on softness, price and the dry feel that a handle wants.
Two of the three also share a weakness in sunlight. Standard TPR and standard TPU both need a stabiliser before they go outdoors, and neither is a roofing material.
A useful check sits on the site already: the comparison of TPU against silicone covers the two harder options in more depth.
Where TPR Fails
Heat is the first limit. A general-purpose grade runs to 60 or 80 °C, and a spatula resting on a pan edge passes that in seconds.
Grease is the second. The butadiene middle absorbs oil, the part swells, and the surface turns sticky to the touch.
Sunlight is the third. Ultraviolet light attacks the same double bonds, so a grip on a garden tool chalks and then cracks.
Set is the fourth. Clamp a TPR part and it slowly loses its push-back, which is what the 60 to 76 % figure above describes at 100 °C.
Smell and stain are the two that never reach a datasheet. Mineral oil can migrate out of a soft compound, and a pale grip can pick up colour from a dark shelf liner.
Heat ageing also changes the feel, not just the shape. A grip that has spent a summer in a car may still fit and still feel wrong.
None of this rules the material out of a kitchen. It rules out a drawing that says only “TPR” and leaves the chemistry open.
Reading The Retail Label
Most people meet this material on a box, not on a datasheet. Four phrases on that box carry most of the weight.
“BPA free” is the easiest to keep. Bisphenol A is not part of the block copolymer, so a plain compound passes without extra work. Colourants and additives still need their own papers.
“Food grade” is a claim about one grade, not about a family. Ask which report covers which part, and read the specimen size and the test conditions on the report.
“TPR grip” says nothing about chemistry. The same words describe a 47 Shore A SEBS grip that lasts and an SBS grip that turns tacky in a year.
“Recyclable” deserves a second question. A TPR part can be melted again, but that says nothing about the collection system where the product is sold.
None of this makes the label dishonest. It makes the label incomplete, and five minutes with the supplier’s papers closes the gap.
What The Food Rules Actually Say
If the grip touches food, two different US rules apply, and a supplier usually quotes only one of them.
The polymer itself is cleared under 21 CFR 177.1810, the section for styrene block polymers. That section prints a minimum molecular weight for each type.
SBS needs 29,000, and the hydrogenated version, listed under CAS 66070-58-4, needs 16,000.
It also prints extractable limits. SBS may give up 0.0039 mg/cm² in refluxing water over 30 minutes, and the hydrogenated grade may give up 0.002 mg/cm² over two hours.
The finished part is covered by the repeated-use rule at 177.2600, which tests the whole article, not just the polymer.
| Rule | What is measured | The limit |
|---|---|---|
| 177.1810, SBS polymer | Extractables in refluxing water, 30 min | 0.0039 mg/cm² |
| 177.1810, hydrogenated polymer | Extractables in refluxing water, 2 h | 0.002 mg/cm² |
| 177.2600, water | Total extractives, first 7 h | 20 mg/in² |
| 177.2600, water | Total extractives, next 2 h | 1 mg/in² |
| 177.2600, n-hexane | Total extractives, first 7 h | 175 mg/in² |
| 177.2600, n-hexane | Total extractives, next 2 h | 4 mg/in² |
| EU 10/2011 | Overall migration into a food simulant | 10 mg/dm² |
| EU 10/2011 | General specific migration limit | 60 mg/kg |
The two rules are not interchangeable. A polymer report tells you what went into the compound, and an article report tells you what comes out of the finished grip.
In Europe the question is scope before it is limits. Regulation 10/2011 covers plastic materials and articles, and recital 7 puts rubbers and silicones outside it.
A thermoplastic rubber is not a cured rubber, so it is normally tested as a plastic. Ask the lab to confirm the class of the grade before a claim goes on the box.
Polycyclic aromatic hydrocarbons are the test that catches a cheap compound. Germany’s GS mark now runs on AfPS GS 2019:01 PAK. It replaced the 2014 version on 1 July 2020 and cut the list from 18 substances to 15.
The limits move with contact. Material put in the mouth allows under 0.2 mg/kg of benzo[a]pyrene. Short contact with skin allows under 1 mg/kg. The sum of 15 PAH runs from 1 to 50 mg/kg.
REACH Annex XVII entry 50 sits next to it. It limits any listed PAH to 1 mg/kg on an article touched by skin, and 0.5 mg/kg for toys.
The wider set of rules, and which documents a kitchenware order needs, is covered in this guide to FDA food contact rules for kitchenware.
The Dishwasher Claim
No public standard sets a cycle count for a TPR handle. Anyone who prints “dishwasher safe” is describing a test they chose themselves.
So the test has to be written into the order. Name the cycle count, the water temperature, the detergent and the pass mark.
A pass mark can stay simple: no peeling from the hard part, no colour shift and no tacky surface.
Two failures appear first. The bond line lifts where the melt never reached the surface, and the oil in a soft compound migrates to the skin.
Both show up long before the part looks worn, so a few hundred cycles in a test kitchen cost less than a container of returns.
Six Lines For The Order
A drawing that says only “TPR” leaves a factory free to pick the cheapest grade that fits the name. Six lines close that gap.
Line one, the chemistry. Write SEBS-based if you want the stable version, because SBS passes the same hardness test and fails in the sun.
Line two, the hardness. Give a target and a tolerance in Shore A, and name the test method, so two labs report the same number.
Line three, the bond. Name the substrate, the peel test and the minimum value in N/mm. A grip without a peel figure is an opinion.
Line four, the set. Put a maximum on compression set after a stated time and temperature, since this is the property that fails quietly.
Line five, the papers. Ask for a 177.1810 report on the polymer and a 177.2600 report on the part, plus a 10/2011 report for the EU.
Line six, the process. No regrind, drying for two to four hours at 60 to 80 °C, and a mould temperature between 40 and 60 °C.
Those six lines fit on one page. They turn a material name into something a factory can accept or reject, and they give an inspector something to measure.
The same page works for any moulded part. The guide to a specification sheet a Chinese factory will sign covers it.
If a soft-grip sample is on your desk, send the datasheet and the peel figure. I will read the chemistry, the Shore A tolerance and the bond to the hard part, then tell you which line a factory is likely to argue about before the tool is cut.
Send The DatasheetQuestions Buyers Ask
Is TPR the same as TPE?
TPE is the family name and TPR is one branch of it, the styrene block copolymer type. In trade both words are used for the same pellets.
Is TPR material safe for food?
Only a grade with the right papers is safe, and the name proves nothing. Ask for a 177.1810 report on the polymer and a 177.2600 report on the part.
Is TPR toxic or BPA free?
The base chemistry has no bisphenol A in it, so a plain TPR compound is normally called BPA free. Colourants and additives still need their own paperwork.
Can TPR go in the dishwasher?
It can survive a wash, but no standard sets a cycle count. Write the temperature, the detergent and the pass mark into the order, then test to it.
Why did the grip go sticky?
A cheap SBS compound met oil, heat or sunlight and started to break down. The oil in the recipe also migrates out over time, and that feels the same.
TPR or silicone for a spatula?
Pick silicone if the edge touches a hot pan, because TPR softens at 60 to 80 °C. Pick TPR if the part is a handle, a foot or a grip.
Questions & Comments
We read every one and reply within 24 hoursWhich grade were you quoted, SEBS or SBS, and what does the grip have to survive? A wash cycle, a hot pan edge and a sunny shelf ask for different compounds.