What Is Crocking: Why Dark Fabric Rubs Off, And How It Is Graded

Alan Xiao, Founder of Sourcing Pioneer
Alan Xiao
· Updated November 11, 2026 · 10 min read

Crocking is colour that rubs off a fabric onto something else.

The word is old, the test is mechanical, and the argument it causes is always the same. A buyer sees a grade on a report. The factory says the same fabric passed last season.

Both can be true, because crocking depends on how wet the rubbing cloth is, which standard was run, and how dark the shade is.

This article covers the two methods buyers name and the machine that runs them. It also covers how the grey scale turns a stain into a grade, and six lines that stop a shade dispute.

A folded dark indigo fabric and a white cotton square showing a faint rub mark on a beige studio surface
A rub mark on a white cloth is the whole evidence. Everything else is how that mark gets graded.

The Short Answer

A coloured surface is pressed and rubbed with a white cotton cloth under a fixed load. Whatever colour moves onto the white cloth is the result.

Do it with a dry cloth and you have the dry grade. Wet the cloth first and you have the wet grade. Both get a number from 1 to 5.

Five means no colour moved. One means a heavy stain. Half steps sit between them, so a report often reads 4-5 or 3-4 rather than a whole number.

The tester is called a crockmeter. It was built to copy the pressure and motion of a human finger. That detail matters: crocking is the failure a customer creates by wearing the garment, not by washing it.

Two causes show up over and over. Dye that never bonded properly and dye that was never washed off the surface. Both leave loose colour where a rubbing cloth can reach it.

Dark and vivid shades are the usual victims, for a plain reason. A deep black or a true red needs more dye on the fibre than a pastel does, so there is more loose colour to lose.

Two Methods, And They Are Not Interchangeable

Most reports name one of two standards. AATCC 8 is the American method and it dominates in North America. ISO 105-X12 is the international one, used across Europe and much of Asia.

They look alike on the bench, and they are not the same test. The wet cloth carries a different amount of water in each, and that single difference moves the grade. A side-by-side of the two methods puts the moisture figures next to each other.

ParameterAATCC 8ISO 105-X12
Term usedCrockingRubbing
Wet cloth moistureAbout 65 % pickupAbout 100 % saturation
Rubbing head16 mm16 mm
Downward load9 N9 N
Rubs per runAbout 10, one per secondSet by the lab and the study
Grading scale1–5 grey scale1–5 grey scale

Read the second row again. A cloth at 65 percent pickup is damp. A cloth at 100 percent is fully wet, and wet cloth pulls dye that dry cloth cannot touch.

That is why a fabric can hold a Grade 4 under the American method and land near Grade 2 under the ISO one. Nothing changed in the factory. The test changed.

There is a third name that appears on printed goods. AATCC 116 uses a rotary vertical crockmeter, built for prints and small panels that will not sit flat on a flat-bed machine.

If a report says “crocking 4” with no method named, it is not a result yet. Ask for the standard, the wet or dry condition, and the lab.

What The Machine Actually Does

The bench tool is simple, and the small details are where results diverge.

A specimen sits on the base, often over a sandpaper pad that stops it shifting. A hand crank drives an arm back and forth over a straight path of about 100 mm.

On the end of that arm is an acrylic finger, 16 mm across, wrapped in white cotton and held by a wire clip. The arm is weighted to press with a constant 9 N.

A mechanical counter records the cycles. At the end, the cloth comes off and the stain is compared with a scale.

Contact area is the quiet variable. An embossed or heavily printed surface touches the cloth on its high points only. A raised pattern can score better than the flat cloth it was printed on.

A seam, a thick hem or a double layer changes the reading too. Labs are supposed to keep the specimen flat and single layer for that reason.

The cloth itself is a specification, not a rag from the cutting room. The instrument maker lists the cloth spec that AATCC 8 calls for: a combed cotton with a bleached, desized finish and no optical brightener.

It sets the fibre staple between 10.3 and 16.8 mm, and a yarn of 15 tex in a plain weave. Mass is about 113 g/m² greige, or 100 g/m² finished.

Two numbers on that list explain a lot of disagreements. The pH is held at 7 ± 0.5, and the whiteness at W = 80 ± 2.

Substitute a whiter cloth and a faint stain looks stronger. Substitute an acidic cloth and the dye behaves differently. Either way the number moves without anything changing in the fabric.

Specimen size is small too, roughly 38 mm by 127 mm, with crocking squares of about 50 mm by 50 mm cut from the roll.

Pile fabrics get a different head. AATCC 165 uses a crock block of 19.0 mm by 25.4 mm. A round finger stains the ring of a tuft more heavily than the middle.

Diagram of a crockmeter: a 16 mm acrylic finger under a 9 N load rubbing a white cotton cloth over a specimen along a 100 mm path
Four numbers define the run: 16 mm head, 9 N load, about 100 mm of travel, and a controlled white cloth.

How A Stain Becomes A Grade

There is no instrument reading here. A trained pair of eyes compares the stained cloth with a set of standard grey chips.

Grade 5 is a cloth with no visible stain. Grade 4 shows a slight change, Grade 3 a noticeable one, and Grade 1 a heavy transfer of colour.

Half steps are normal. A lab reports 4-5 when the stain sits between the Grade 4 chip and a clean cloth. A 3-4 sits between three and four.

Because the judgement is visual, the light matters. Good labs grade in a light booth under a stated illuminant, at a stated angle, with the cloth flat.

Two labs can still differ by half a grade on the same fabric. That is not dishonesty. It is the width of the method.

So a report is worth more when it states the conditions: which grey scale, which light source, and who read it. A bare number loses half its meaning.

Some labs now add an instrument reading to support the visual call. A small bench spectrophotometer measures the stain, then the operator still decides. It narrows the gap between two labs, and it does not remove it.

The scale also has a ceiling effect worth knowing. A Grade 5 does not prove the fabric will never crock. It says nothing moved under that load, that moisture level and that number of rubs.

Raise the moisture to a fully wet cloth, as the ISO method does, and some of those Grade 5 fabrics will show colour.

Where The Loose Colour Comes From

Almost every crocking failure traces back to colour that sits on the surface instead of inside the fibre.

Dye that never bonded. The dye molecule needs time, heat and the right chemistry to fix to the fibre. A short dwell or a cold bath leaves it half attached, and rubbing lifts it.

Dye that was never washed out. Even a well-bonded dye leaves surplus on the surface after the dye bath. Soaping and rinsing clear it. Skipping that step saves water and costs you the grade.

Pigment printing. Prints do not dye the fibre at all. A pigment is glued to the surface by a binder. The print sits above the fibre, so a rubbing cloth reaches it first.

That gives a useful field clue. A fabric that is lighter on the reverse side than the face is usually a surface print or a surface dye. Both types crock.

A weak binder or an under-cured print. Too much pigment for the amount of binder leaves dry colour on the surface. A print that was not cured long enough behaves the same way.

Leather and coated surfaces. The finish on a leather or a coated fabric is a film. If the finish coat is thin or poorly fixed, it transfers on to whatever rubs against it.

Too much softener. A soft handle sells, but lubricating the fibre also helps dye slide off it. This is one of the quieter trades in finishing.

Why Dark And Vivid Shades Fail Most

A deep black needs a heavy dye load to reach the shade. A pale grey needs very little.

More dye in the bath means more dye left near the surface, and that is the layer a rub can reach. The same logic runs through navy, deep red, forest green and any true black.

Indigo is the extreme case, because the dye sits on the yarn rather than inside it. It is also the reason dark denim has a reputation for marking pale leather and light upholstery.

So the risk is not the shade itself. It is the gap between how much dye the shade needs and how well the factory fixed and washed it.

This is why a Grade 4 on a pastel tells you very little about the same mill’s black. Ask for the report on the actual colour you are ordering, not on the base cloth.

Roll to roll variation is the other half. Two rolls of the same shade can differ if the dye bath was refilled between them. One passing swatch does not clear a whole shipment.

The Numbers A Buyer Will Ask For

No law sets a crocking grade. What exists is a set of trade criteria, agreed by segment, and most contracts copy one of them.

The table below is the set published for contract textiles. It is the set quoted most often in upholstery and drapery. It also shows how the wet number is treated more loosely than the dry one.

ProductDry, minimumWet, minimum
Upholstery, woven (AATCC 8)Grade 4Grade 3
Upholstery, coated (AATCC 8)Grade 4Grade 4
Drapery, solid (AATCC 8)Grade 3Grade 3
Drapery, print (AATCC 116)Grade 3Grade 3
Wallcovering, direct glueGrade 3Grade 3
Wrapped panels, upholstered wallsGrade 3Grade 3

Read the coated row. A coated fabric is asked for Grade 4 wet, the same as dry. A film finish that moves colour under moisture has nowhere to hide.

Illustrative five step grey scale for staining, from grade 5 with no transfer to grade 1 with heavy transfer, with the usual contract cut-offs marked
Five steps, plus half steps in practice. The cut-offs on the right are the contract figures, not a legal limit.

Apparel contracts usually set their own line. A common pair is Grade 4 dry and Grade 3 wet, and a brand selling to a hot, humid market often lifts the wet figure.

None of these numbers mean anything without the method. A Grade 3 under ISO is not the same product as a Grade 3 under AATCC 8, because the wet cloth was wetter.

Wet Crocking Is The Hard One

Water weakens the bond between dye and fibre, then acts as a carrier for whatever comes loose.

That is why a wet grade is nearly always the lower of the two. It is also why a fabric that passes dry can mark a pale shirt on a humid day.

It is also why the moisture figure matters so much. At about 65 percent pickup the cloth is damp. At 100 percent it is saturated, and the same fabric can fall two grades.

Ask how the wet cloth is prepared. A lab that wets a cloth and squeezes it by hand is close to the American method. A lab that soaks it to saturation is running the ISO one, and its numbers will run lower.

For a factory, this is the useful pressure point. If the wet grade is the one at risk, the fix is usually more washing and better fixation, not a different dye colour.

Fixing It At The Factory

The fix is almost always a process step, not a new colour. Four levers cover most cases.

Wash off properly. Soap the goods after dyeing and rinse until the water runs clear. This is the cheapest lever and the one most often cut when a mill is behind schedule.

Fix the dye. The right chemistry, the right dwell time and the right temperature decide how much dye actually attaches. A shade can look right and still be half fixed.

Rebalance the print paste. More binder, or a crosslinker, or a longer cure, keeps pigment on the fabric instead of on the rub cloth.

Ease off the softener. A softer handle can be bought with a lower crocking grade. Asking for both is legitimate, and it costs money.

The order of work matters. Test a lab dip before the bulk run, on the actual shade, and test both dry and wet. A dry result alone will not catch the failure a customer creates with a sweaty hand.

If the mill cannot show a wet figure for the shade you are ordering, the safest assumption is that nobody has looked.

Six Lines For The Order Sheet

Six lines turn “crocking 4” into a clause a factory can be held to.

One, the standard. AATCC 8 or ISO 105-X12, written in full. Never a bare grade.

Two, dry and wet as separate lines. They are two results, and the wet one is the one that fails.

Three, the shade and the substrate. The report must describe the colour you are buying, on the fabric you are buying, not a base cloth.

Four, the specimen. State that the report covers the production weight and finish, because a washed or softened sample is a different material.

Five, the lab and the report number. A grade without a traceable report is a sentence, not evidence.

Six, the retest trigger. A new dye lot, a new mill or a new finish should pull a fresh test.

All six belong in the tech pack the mill works from, next to the shade band and the fabric weight. Weight per square metre is the same measure a mill already quotes, so the two sit naturally together.

Write them into the one-page brief the factory signs off before sampling starts, then hold the bulk to the same page.

When the goods are packed, a check on the finished run should pull a swatch for the file. The colour that ships should match the colour that was graded.

Six numbered clauses for a crocking requirement on an order sheet, from the standard to the retest trigger
Six clauses. Each one closes a way a grade can be quoted and then quietly not met.
SEND THE SWATCH

Send the test report and the shade you are ordering. I will check which method was run and how wet the cloth was. I will also compare the sample with the bulk you will receive, then tell you which line is missing.

Ask For A Report Check
Is crocking the same as bleeding?

No. Crocking is colour that moves by rubbing. Bleeding is colour that moves into water during washing. A fabric can do one without the other, and they are tested separately.

What is a good crocking grade?

Grade 4 or better dry is the usual ask for apparel and upholstery. Wet is judged more loosely on woven goods, at Grade 3, and more strictly on coated ones, at Grade 4.

Why does my black fabric fail when the navy passes?

Black needs a heavier dye load, so more colour sits near the surface where a rub can reach it. Same mill, same process, different amount of dye to fix and wash out.

Can I compare an AATCC 8 result with an ISO 105-X12 result?

Not directly. The ISO wet cloth is saturated, the AATCC one is damp, so the same fabric often scores lower under ISO. Compare results from the same method only.

Does washing improve a low grade?

Often yes, once. A home wash removes loose surface dye, which is why a garment can mark on the first wearing and stop later. It is not a fix for dye that never bonded.

How long does the test take?

The rubbing itself is quick, about ten cycles. Conditioning, wetting to a set pickup, drying and grading are what fill the day. Plan a few days per submission.

Questions & Comments

We read every one and reply within 24 hours

If a crocking report lands on your desk, send it over. I will read the method, the dry and wet figures, and whether the swatch was the shade you are buying.

Subscribe
Notify of
guest
0 Comments
Most Voted
Newest Oldest
0
Would love your thoughts, please comment.x
()
x