What Is Conformal Coating: A Barrier, Not a Finish
Conformal coating is a thin plastic film over a finished board. It follows every part, and it is not a paint job.
The word conformal means it takes the shape of what it covers. The film is tens to a couple of hundred micrometres thick.
It is not a metal finish, not a fabric treatment, and not potting compound. Those are three other processes with three other bills.
What it does is narrower and more useful than “protection”. It keeps the wrong chemistry away from the wrong place.
The Short Answer
Conformal coating is a protective polymer layer applied to an assembled circuit board after soldering and cleaning.
It is sprayed, brushed, dipped or deposited in a vacuum, then cured. The result is a continuous film over the components and the joints.
Typical thickness runs from about 25 to 250 microns depending on the method and the chemistry. A hair is roughly seventy.
The film is applied to the assembly the coat goes onto. That is why the coating step sits at the end of the line, not the start.
One thing it is not. A coating is not a seal. Most chemistries let water vapour pass, which the next section explains.
What It Actually Stops
The intuitive story is wrong, and the correct one is more useful. A conformal film is not a waterproof bag around the circuit.
Apart from one resin, these films are penetrated by water molecules quite easily, as the reference on conformal coating puts it. Water alone is not what kills a board.
What kills it is water plus salt. Dust, fingerprints and flux residue leave ions on the surface, and damp air turns them into a microscopic electrolyte.
That film of salty water bridges two nodes that should be separate. The result is leakage, drift and eventually corrosion.
The coating blocks the ions, not the water. It is a barrier against dirt, and that is why it works even when it is damp.
Three smaller jobs come with the same film. It dampens vibration, it raises the breakdown voltage of a dense assembly, and it can slow the growth of metal whiskers between fine pitches.
That last one is why the aerospace and automotive trades specify it. A whisker is a short circuit that grows on its own.
There is a consequence, and it runs through the rest of this article. If the coating blocks ions rather than water, then whatever is under it stays there.
Flux residue trapped under a coat is worse than flux residue left in the open, because nothing can wash it away afterwards.
Four Chemistries and a Fifth
The four ordinary resins are applied wet and then cured. The fifth is deposited as a gas and needs no curing at all.
The figures below come from a conservation materials database, which compares them on the same axes. Transmission is water vapour, and lower means more resistance to damp.
| Chemistry | Water vapour | Service limit | Film | Can it be removed? |
|---|---|---|---|---|
| Acrylic | 15.9 | 82 °C | 0.03–0.13 mm | Yes, easily |
| Polyurethane | 0.9–3.4 | 121 °C | 0.03–0.13 mm | No |
| Epoxy | 0.94 | 177 °C | 0.03–0.13 mm | No |
| Silicone | 1.7–47.5 | 260 °C | 0.05–0.21 mm | Sometimes |
| Parylene | 0.59 | 60–70 °C | 0.01–0.05 mm | No |
The last column decides more projects than the first. A board that may need rework wants a film that comes off.
Acrylic is the cheap, forgiving choice. It dries to the touch in minutes, cures in a day, and a solvent takes it off a joint in seconds.
Polyurethane and epoxy resist chemicals and abrasion. They stay put. Removing them damages what is underneath. That is the point, and the problem.
Silicone holds its properties across the widest temperature range. It stays flexible, so it survives vibration and thermal cycling. It is also soft, thick, and easy to scuff.
Parylene is the odd one. It is deposited in a vacuum, molecule by molecule. That covers edges and crevices a spray cannot reach, at a fraction of the thickness.
It is also the hardest to remove and the slowest to apply. Vacuum deposition is a batch process, and one chart in the reference notes it does not suit high volume.
Brush, Dip, Spray, Vapour
Four methods, and the choice is made by volume and geometry rather than by preference.
Brush is a person with a brush. It suits prototypes, repairs and awkward shapes, and it depends on the skill of that person. Thickness varies and bubbles happen.
Dip is the fastest way to coat many boards. The variables are how fast the board goes in, how fast it comes out, and how thick the liquid is.
Its weakness is that liquid goes everywhere, including under components. A design with parts that must stay dry underneath is not a dip design.
Spray covers the middle ground and is easy to automate. Solvent mix, nozzle pressure and spray pattern are the settings, and the shadow behind tall parts is the limit.
Selective machines use a needle or a narrow spray head that follows a program. They coat only where the drawing says. That is how high volume avoids most masking.
Vapour deposition is the fifth. The material is heated, becomes a gas, and settles on every exposed surface in the chamber.
That evenness is the selling point. The cost is the chamber, the batch, and masking that must be air-tight rather than stuck down.
The Masking Nobody Quotes
Anything that must make electrical contact afterwards has to stay bare. Connectors, test points, battery contacts, switches and mating surfaces all fall in that group.
Every one of them is a keep-out area, and keeping it clear is a manual step. Somebody tapes, plugs or caps each one before the board is coated, as a coating house’s process guide describes.
That work has a drawing of its own. The masking drawing states what is covered and what is not. The finished masking is checked against it before coating starts.
It also has a failure mode. Tape that lifts at an edge lets coating bleed underneath, and a connector with coating in it is a connector that no longer works.
Then there is the other end. The masking has to come off while the film is firm but still soft, or de-masking tears the coating around the opening.
A leak costs a repair. The coating is stripped locally, the component is cleaned or replaced, and the area is re-coated and re-inspected.
So the masking is labour, plus inspection, plus a drawing that has to be maintained as the board changes. It is the line a coating quotation usually omits.
Cleanliness Comes First
The coating step has one prerequisite, and it happens before the coating. The board has to be clean.
Flux residue, dust and the salts from a fingerprint all sit on the surface. Under a film they stay there, and damp air will find them.
A pinhole is the mechanism. Every film has thin spots, and a thin spot over a contaminated area completes the circuit that the coating was meant to break.
So the process starts with a cleanliness check rather than a coating. If the board fails it, the board is washed and checked again.
This is the same wash decision that follows assembly. It is why a no-clean process and a coating step belong in the same meeting.
Coating over residue is not a shortcut. It locks the contamination in place for the life of the product, where nothing can wash it out.
Cure Is Part of the Spec
A wet film is not a coating yet. It becomes one when it dries or reacts. The difference between routes is measured in days.
An acrylic is dry to the touch in about ten minutes and properly cured within a day. That speed is a large part of why it is the default choice.
A polyurethane can take from one day to a month to reach its final state, depending on the formulation and the room.
Silicone usually cures within an hour, which is quick for a material that tolerates the highest service temperature in the table.
Two routes skip the wait entirely. Ultraviolet curing sets a film in seconds under a lamp. That is why automotive and consumer lines use it.
Vapour deposition has nothing to cure. The film is finished when the batch comes out of the chamber.
Whatever the route, the cure belongs in the specification. A board packed before it is cured is a board whose film is still moving.
How You Know It Is There
A transparent film on a busy board is hard to see. That is why nearly every modern coating carries a fluorescent dye.
Under a long-wave ultraviolet lamp, the film glows and a bare patch does not. Checking under a lamp is the traditional method, and cameras are replacing it.
Coverage is only half of it. Thickness is measured, and the method depends on whether the film is wet.
A wet film gauge is a comb pressed into the fresh coating. The teeth show how deep it went. A dry film is measured with eddy currents.
Both methods want a witness. A coupon coated alongside the boards is easier to measure. It is also easier to cut open.
The figures to hold come from the standards: 30 to 130 micrometres for acrylic, epoxy and urethane, and 50 to 210 for silicone.
The same standards name the defects, and dewetting is the one to know by name. The film pulls back from a surface instead of covering it, and it looks like a clean patch in the wrong place.
The acceptability standard that names dewetting is the document to cite in an order, because “coated” without it means whatever the operator thought.
Five Lines That Define the Job
A coating order is a specification before it is a price. Five lines decide whether the result can be checked at all.
| Line | What to write | What goes wrong without it |
|---|---|---|
| Chemistry and thickness | The material, and the film thickness after cure | Thin coverage passes a look and fails a humid week |
| Keep-out list | Every area that must stay bare, on a masking drawing | Coating creeps into a connector |
| Cleanliness | The test and the limit, before coating | Residue is sealed in for the product’s life |
| Cure | The route, the temperature and the time | Boards are packed while the film is still moving |
| Inspection | UV coverage, thickness method, and the standard cited | Nobody can prove the film is where it should be |
The second line is the one that shows up as a defect, because a masked opening is either clear or it is not.
The fifth line settles arguments. A named standard and a named measurement turn “it looks coated” into a pass or a fail.
Sealing is a related question with a different answer. The rating that answers a different question is about a whole enclosure keeping water out, not a film deciding what reaches a joint.
For a comparison across suppliers, the answers need to line up. One sheet with the coating on it does that better than four data sheets in four layouts.
Six Lines for the Order
Put the five lines into six sentences, and the coating stops being a step somebody adds at the end of the quotation.
One. Name the chemistry, the method and the thickness after cure.
Two. Attach a masking drawing that lists every keep-out area, and require it to be inspected.
Three. State the cleanliness test and its limit, and who pays for the wash if it fails.
Four. Give the cure route, the temperature and the minimum time before packing.
Five. Name the inspection: UV coverage, thickness method, and the standard the work is judged against.
Six. Agree the rework policy, including who owns a board with coating in a connector.
The sixth line is where the masking cost finally lands on paper. A leak is not a mystery; it is a labour hour and a decision about the board.
Before the order grows, look at the goods. The market where coated boards are traded is a place to see coverage under a torch, which is the only honest test at a counter.
None of that replaces a look at the line. A line visit that opens the coating booth should include the masking bench and the UV lamp.
Send me the coating specification you were quoted and I will read the five lines. I will say which chemistry was chosen and why it matters, whether the keep-outs are listed, and where the masking cost has been left out. No cost, no obligation.
Check My SpecQuestions Buyers Ask
Is conformal coating waterproofing?
Not in the way buyers imagine. Most chemistries let water vapour through. The film blocks salts and other ions, which is what turns damp air into a conductive path.
What is the difference between coating and potting?
Potting fills a cavity with resin so the board sits inside a solid block. Conformal coating is a thin film over the surface that follows every part.
Which chemistry should I choose?
Start from the rework question. Acrylic comes off easily, polyurethane and epoxy do not, and silicone sits in between. Temperature and chemical exposure then narrow the choice.
Why is masking such a large part of the cost?
Because it is done by hand, checked against a drawing, and removed at the right moment. Every connector and test point on the board adds to that work.
Can a coated board be repaired?
Yes, by stripping the film locally, repairing the joint and re-coating. How hard that is depends on the chemistry, and on parylene it is a workshop job.
How thick should the coating be?
The standards give ranges: about 30 to 130 micrometres for acrylic, epoxy and urethane, and 50 to 210 for silicone. What matters is that the range is written down and measured.
Questions & Comments
We read every one and reply within 24 hoursIf a board came back with coating inside a connector, send me the masking drawing. That drawing is where the defect was decided.