Lost Wax Casting Jewelry: Where The Tooling Fee Lands
Lost wax casting is a jewelry process where a wax model is sealed in plaster, burned out, and replaced by molten metal. The tooling fee on the first order pays for the model and the rubber mold, not the castings.
Buyers usually meet this process as a line item. The quotation says mold fee, or tooling, or development, and the number is either small enough to ignore or large enough to stop the order.
What sits behind that line is a fixed sequence. A master model is made. A rubber mold is cut around it. Wax copies are injected, joined to a sprue, invested in plaster, baked, and cast.
Only part of that work repeats with every run. The rest is paid once, and that split is what a buyer needs before agreeing to any fee.
What The Fee Actually Buys
The tooling fee usually covers three things: the master model, the rubber mold, and the first cast sample.
The master is the original. It can be grown from a CAD file, printed in castable resin, or carved by hand. It is the only item that defines the design, so it is also the item that a change request destroys.
The rubber mold is made by packing the master in uncured rubber and heating it under pressure. Once cured, the rubber is cut open, the master is removed, and the cavity left behind becomes the production tool.
A mold is cut for one size and one shape. A second size needs a second mold, even when the design is identical.
The third item is the sample. Someone has to cast one, clean it, and check it before the mold is accepted. That labour sits in the fee as well.
None of these three scale with order quantity. A run of 50 pieces and a run of 5,000 use the same mold, which is why the fee looks heavy on a small order and trivial on a large one.
Why The Tree Matters More Than The Mold
Wax copies are joined to a central wax sprue, and the result is called a tree. Every piece on that tree is fed through one channel.
Sprue placement decides whether a casting fills. The rule in every workshop is the same: attach at the thickest section, and let the metal reach the thin edges last.
Put the sprue on a thin band and the metal freezes before the far side fills. The result is a short fill, and the piece is scrap before it reaches finishing.
A tree also sets the batch size. Flasks come in standard diameters, and a tree that fits loosely wastes plaster; a tree packed too tightly traps gas and produces porosity.
Mold life belongs here too. Rubber takes wear at every injection, so a mold that has produced thousands of waxes will start to lose sharpness on fine detail. Reputation for “the second order looked softer” usually traces back to the mold, not to the metal.
Six Hours In A Kiln, And Why Nobody Quotes It
Investment is a plaster. It sets around the tree, then has to lose its water, its wax and its carbon before metal can enter.
That happens on a ramp, not in one step. Heat too fast and trapped steam cracks the mold, and cracks become fins of metal on the finished piece.
A published jewellery schedule runs in four stages, and the temperatures are worth knowing because they explain most casting faults.
| Stage | Temperature | What it does |
|---|---|---|
| Low ramp | Room to about 150 C | Drives off free water slowly, before steam builds |
| Wax out | 150 C to about 370 C | Wax melts and drains through the sprue opening |
| Carbon burn | 370 C to 650-730 C | Oxidises the residue left in the plaster, with air present |
| Final soak | 650 C to 730 C | Holds even heat through the flask until the pour |
The whole programme takes six to twelve hours depending on flask size, plaster type, alloy and kiln load.
There is a hard ceiling near 750 C. Past it the gypsum in the plaster breaks down and gives off sulphur, which stains and embrittles the metal.
Platinum needs a different plaster. Phosphate-bonded investment survives above 900 C without breaking down, which is why the same workshop runs two materials and two schedules.
For a buyer, kiln time is the invisible cost. A flask cannot be hurried, and a factory running a full kiln every night is running a fixed cycle whether the order is 20 pieces or 200.
The Alloy Decides Half The Risk
Melting points differ enough to change the whole setup. Fourteen karat gold melts near 898 C, sterling near 893 C, and platinum near 1,768 C.
Sterling carries a specific problem. The copper in the alloy oxidises during the pour and leaves fire scale, a grey skin that has to be pickled off before polishing.
Silver also catches gas. A flask that is too cool, or a sprue that is too thin, shows it as porosity under the surface, and porosity only appears after polishing opens it.
Metal accounting is the other half. Castings come off the tree with a sprue attached, and the sprue returns to the crucible. The metal weight on the invoice should say whether returns are credited and at what rate.
That single line explains most of the gap between two casting quotes that look identical on the surface.
Four Faults, Four Causes
Porosity comes from carbon residue or trapped gas. It points at a short burnout, a cold flask, or a tree packed too tightly for air to move.
Flash comes from a cracked mold. The cause is usually a ramp that ran too fast through the water or through the cristobalite inversion near 200 to 270 C.
A short fill means the metal chilled before it reached the end of the cavity. The flask was too cold, or the sprue was attached at a thin section.
Sulphur staining is a high-temperature fault. It appears when gypsum-bonded plaster is pushed past its ceiling, and it cannot be polished out.
All four are process faults, which matters commercially. A buyer who can name the fault can argue about remake cost, and a buyer who cannot is left with a general complaint about quality.
Once Or Per Run, Line By Line
The fee argument gets easier when the whole job is split into two columns. Everything paid once belongs to the design; everything paid per run belongs to the volume.
| Line | Paid once or per run | What moves it |
|---|---|---|
| Master model | Once | Design changes, CAD repair, hand carving |
| Rubber mold | Once per size | Number of sizes, mold life, detail level |
| Wax injection and tree | Per run | Piece count, tree density, tree build labour |
| Plaster and flask | Per run | Flask diameter, yield per flask |
| Burnout | Per run | Kiln hours, load factor, schedule length |
| Metal | Per run, less returns | Piece weight, alloy, sprue credit rate |
| Finishing and setting | Per run | Detail, stone count, plating |
Two lines in that table cause most of the disputes. The first is mold ownership: who keeps the rubber when the order ends.
Ask before paying. A factory that keeps the mold can quote the second order from a position of strength, and moving to another supplier means paying again.
The second is sprue credit. Metal that comes back to the crucible is metal the buyer has already paid for, so the rate matters on every order.
The wider casting supply chain is worth reading before the first quote lands, because the same fee vocabulary appears in every factory.
Reading A Casting Quote
A quote that puts tooling and pieces in one number cannot be compared with anything. Ask for the two figures apart, even when the supplier resists.
Then ask what triggers a remake. Most factories will remake a fault they caused, and most will charge for a fault the buyer caused in design.
The line between the two is the approved sample. Once a sample is signed, every later argument is measured against it, so the approval step is worth more care than the price negotiation.
Ask for the sample in the production alloy, not in a bench alloy, and judge it after polishing. Porosity that hides in a matte casting shows up under a mirror finish.
Volume thresholds belong in the same conversation. Tooling is often waived above a quantity, and that cut-off is a negotiating point rather than a rule.
Finally, ask for the mold life in pieces. A number turns “the second batch looked softer” into a maintenance question with a date attached.
What To Inspect On The First Article
Weigh the sample against the wax. The difference shows how the shrink was compensated, and an unexpected gap means the master was scaled by habit rather than by alloy.
Measure three features with a caliper: the band width, the setting opening and the overall length. Castings drift where the metal is thickest.
Look at the surface under ten times magnification before plating. Pits and pinholes are porosity, and plating makes them worse rather than hiding them.
Check where the sprue was cut. A sprue mark on a visible face is a finishing cost that someone has to pay on every piece.
Confirm the fire scale is gone on silver, since a pickled surface that was rushed will show as a cloudy patch after polishing.
Then send the approved sample for an inspection before the bulk run leaves, so the reference stays in the factory as well as in your drawer.
From A File To A Master
Most designs now arrive as a CAD file, and the file is not the master. A printer turns it into a resin pattern, and the foundry decides what to do with it.
Resin patterns can be cast directly, but the burnout has to change. Castable resin leaves more ash than wax, so the ramp starts slower and the final soak runs hotter and longer.
The other route is the traditional one. Print the pattern, mould it in rubber, inject wax, and cast the wax. It costs an extra mould, and it buys a production tool that can make thousands of copies.
That choice is the hidden line in a tooling quote. A quote built on direct resin casting has no rubber mould, and it cannot repeat the piece cheaply later.
Ask which route the fee assumes. A supplier who cannot answer is usually quoting the cheapest path and hoping the volume never arrives.
When Casting Is The Wrong Answer
Casting wins on complex shapes and on repeat copies. It loses on three cases, and a buyer should know them before paying for a mould.
The first is a one-off. A single ring in a soft design can be made by hand from sheet and wire for less than a mould costs.
The second is a piece that will change every season. A fashion line that redraws its range twice a year pays for a new master each time, and the mould never earns back its cost.
The third is a design that needs spring in the metal. Cast metal is weaker than worked metal, so a thin clasp or a light ear wire is better fabricated than cast.
A hollow form with a wall too thin to cast belongs in the same list, because the metal will not fill it.
None of that makes casting a bad choice. It makes the fee a decision rather than a formality, which is the whole point of reading it line by line.
Six Lines For The Order Sheet
Tooling, separately. Master, mold and sample as three figures, not one.
Mold ownership. Who keeps it, and what a transfer costs.
Mold life. Expected waxes per cavity, in pieces.
Sprue credit. The rate, and whether it is per gram or per piece.
Alloy and finish. The exact alloy, plus the finish the sample was judged in.
Remake terms. Who pays, and against which approved sample. A written spec sheet keeps that reference stable across batches.
Send me a casting and tooling quotation with the mold fee broken out. I will separate the once-only lines from the per-run lines, check the sprue credit and the mold life, and tell you which numbers to fix before the first batch. No cost, no obligation.
Break Down My QuoteQuestions Buyers Ask
Is lost wax casting the same as investment casting?
In jewelry, yes. The trade uses both names for the same route: a wax pattern is coated in plaster, the wax is burned away, and metal takes its place.
How much does the tooling cost?
It depends on the master, the number of sizes and the detail level, so no public price list exists. Ask for the three figures apart and compare like with like.
Why does a second size need a new mold?
A mold holds one cavity at one size. Scaling the design means a new master and a new cavity, even when nothing else changes.
Can a casting be repaired instead of remade?
Small pits can be filled and polished, and a short fill cannot. Porosity that runs through a shank is a remake, not a repair.
Does the metal weight change after casting?
Yes. The piece shrinks as it solidifies, and the master is scaled up to compensate. Weigh the sample rather than trusting the estimate.
How long does the first order take?
Model and mold work is measured in days, and the casting cycle itself includes a six to twelve hour kiln run. Finishing after that is the variable.
Questions & Comments
We read every one and reply within 24 hoursSend the numbers, not the adjectives. I read casting and tooling quotes line by line, and I answer every question below in the language you wrote in.