What Is Zamak: Four Grades, One Impurity Line

Alan Xiao, Founder of Sourcing Pioneer
Alan Xiao Founder of Sourcing Pioneer
· Updated November 16, 2026 · 11 min read

Zamak is a zinc alloy with four percent aluminium.

The name is an acronym of four German words: Zink, Aluminium, Magnesium and Kupfer. New Jersey Zinc developed the family in 1929, and it has been the default metal for cast fittings ever since.

Most of what a buyer meets as a cast pendant, a zipper pull, a buckle, a bag hook or a bathroom fitting is zamak. It melts low, fills a mould well, and takes plating.

This article gives the four grades. It covers the impurity line that decides whether a lot survives five years. Then the six lines that belong on a drawing.

Studio still life on beige of two zamak castings, a pendant and a buckle, one raw and one gold plated
Same alloy, two finishes. The metal is cheap; the finish is not.

The Short Answer

Zamak sits inside the zinc-aluminium family. One rule separates it from the rest of that family: every zamak grade carries about 4 percent aluminium.

The aluminium does the hard work. It gives the melt enough fluidity to fill a thin cavity, and it holds the cast part to a stable size after it cools.

Magnesium is a fraction of a percent. It controls grain growth and keeps the alloy from turning brittle in the pot.

Copper is the variable. Each grade adds a different amount, and that single number sets the strength and the ductility.

So “is it zamak” is the easy question. “Which zamak” is the one that changes the price, the thin wall and the failure mode.

Four Grades On One Shelf

Zamak 3 is the reference grade. It is the base composition of the family, roughly 96 percent zinc and 4 percent aluminium. It is also the most cast grade in North America.

Zamak 5 adds copper. The result is around ten percent stronger and harder, with slightly better corrosion behaviour and less ductility. It is the grade Europe reaches for.

Zamak 2 adds three times as much copper again. It is the strongest and the most brittle of the family, and in a gravity-cast form it is known as Kirksite and used for tooling.

Zamak 7 goes the other way. It carries less magnesium and a small nickel addition, which buys fluidity and ductility for thin walls, at the cost of tensile strength.

GradeCopperTensile strengthElongationChosen for
Zamak 22.6 to 2.9%397 MPa6%Strength and hardness
Zamak 30.25% max268 MPa6.3%Castability, stable size
Zamak 50.75 to 1.25%331 MPa3.6%Strength with plating
Zamak 70.25% max285 MPa14%Thin walls, bending
Chart of the four zamak grades showing copper content against tensile strength and elongation, with Zamak 2 strongest and Zamak 7 most ductile
Four grades, one aluminium figure. Copper is the dial that moves strength.

The elongation column is the one to read twice. A pendant that will be dropped wants the ductility of grade 7 or the balance of grade 3, not the hardness of grade 2.

There is a fourth grade in Asia, Zamak 4, which carries about half the copper of grade 5 to reduce sticking in the die. A quote from one region and a quote from another may quietly use different alloys.

Zinc Pest, And Why Impurities Matter More Than Strength

Early zinc castings failed in a way that has a name. Parts swelled, cracked along the grain and crumbled to grey powder, years after they were shipped.

The cause was not zinc. It was lead, cadmium and tin at levels too low to see on an order sheet and high enough to start intergranular corrosion.

Zamak solved it with purity. The process depended on 99.99 percent zinc, and the alloy family has carried impurity limits ever since.

Those limits are the real specification. Under ASTM B86 for cast Zamak 3, lead is capped at 0.005 percent, cadmium at 0.004, tin at 0.003 and iron at 0.1.

Bars comparing the 0.25 percent copper allowance with the lead, cadmium, tin and iron caps for Zamak 3
The alloy is allowed a quarter of a percent. The impurities get thousandths.

Compare that with the copper allowance, which is 0.25 percent. The impurities are limited twenty to eighty times tighter than the alloying element, and for good reason.

A batch that tests inside the copper range but carries 0.02 percent lead will look perfect at goods-in. It will fail in a customer’s hands two winters later, and the return will arrive long after the balance is paid.

The Two Columns On A Drawing

A zamak part is specified twice: once as metal, once as a casting.

The ingot is covered by ASTM B240 in the United States and EN 1774 in Europe. The casting is covered by ASTM B86 and EN 12844. National equivalents include GB 8738 in China, and JIS H 5301 in Japan.

The difference is not paperwork. An ingot standard fixes what goes into the pot; a casting standard fixes what comes out, including the mechanical results the buyer can test.

In practice the drawing needs both columns plus the tests. Grade and standard, the mechanical values that follow from it, and the impurity caps that decide whether the lot ages well.

One page of that is worth more than a thousand words of email, and the same one page is what a factory builds to.

Why It Casts So Well

Zamak solidifies between about 381 and 387 degrees Celsius. That is low enough for a hot-chamber machine, where the injection cylinder sits in the melt itself.

A hot chamber runs faster than a cold chamber, because the metal does not have to be ladled into a sleeve for each shot. Cycle time drops, and the die stays cooler.

Zinc is also gentle on tooling. A steel die running zamak lasts far longer than the same die running aluminium. That is why the tooling cost per part falls quickly on a long run.

The wall is the part that decides quality. Zamak fills a thin section well. A section thinner than the design allows will show cold shuts and laps, and polishing does not hide them.

Trimming is the other cost inside the cycle. Runners and flash come off by hand or in a trim die. A part with thin petals needs the die, not a knife.

Grade 7 exists for exactly that case. Its lower magnesium and extra nickel buy fluidity, so a pendant with thin flower petals can be cast in one shot instead of two.

Plating, Paint, Chromate

Zamak takes a finish better than most casting alloys. It can be electroplated, wet painted, or given a chromate conversion coat.

Plating is the usual route for jewellery, zipper hardware and buckles, because a polished zamak surface plates bright and holds the shine.

The enemy is porosity. Gas trapped under the skin opens as a blister in the plating bath. That blister is a reject which only appears after the expensive step.

Two controls reduce it. Cast with a die that vents properly, and bake the parts before plating so that trapped gas leaves early.

For anything worn against skin, the finish carries a second duty. Nickel release must stay under 0.5 micrograms per square centimetre per week, tested to EN 1811, and the report has to name the parts tested.

The quality of the plate is not the only variable. A plated casting can pass a thickness check and still fail on adhesion, which is why a tape test belongs beside the micrometer.

Two Edges Worth Knowing

The first edge is temperature. The strength figures on a data sheet are room-temperature values, and zinc alloys lose strength as the part gets warmer.

That does not make zamak unsuitable for a buckle or a pendant. It does mean a load-bearing bracket near a motor needs a figure at working temperature, not a figure at 20 degrees.

The second edge is the joint. Zamak is cast, not welded, and a repair weld on a thin casting usually creates more porosity than it closes.

Cleaning is the other everyday limit. Zinc reacts with strong acids and strong alkalis. A chlorine bleach or a descaling cleaner will dull a bare casting and can lift plating at an edge.

A mild soap, a soft cloth and a dry finish are enough. That instruction belongs on the card, because the customer who reads it is the one who keeps the part.

Where a part must carry load and take heat, the answer is usually a different alloy rather than a thicker zamak section.

Against The Alternatives

Four metals meet in the same quotation, and the choice is rarely about strength alone.

MetalCast thinPlates wellWeight for sizeWhere it wins
ZamakYesVery wellHeavyComplex shapes at volume
BrassFairVery wellHeavierMachined and turned parts
AluminiumFairPoorlyLightLarge parts, low weight
SteelNoWellHeavyStrength and thin sections

Zamak’s advantage is shape. A pendant with a modelled face, a buckle with a logo in relief, a hook with an undercut: these are casting shapes. Casting shapes are where zamak is cheapest.

Its disadvantage is weight and finish dependency. A zamak part is heavy for its size, and it always needs something on the surface before it can be sold.

Brass behaves like a better zamak and costs more. Aluminium is light and awkward to plate, which rules it out for most gold-coloured jewellery. Steel is strong and cannot be cast into these shapes at all.

Five Checks At Goods-In

Weight per piece against the drawing. A light part usually means a short shot or a thinner wall than agreed.

Critical dimensions on the features that mate with something else: the hook opening, the hinge, the pin hole.

Drop from a stated height onto a hard floor, in the packed state, with the failure recorded rather than judged.

Plating by thickness on the wear face, plus a tape test for adhesion and a look for blisters after a warm soak.

Composition by X-ray on a sample, aimed at the impurity elements rather than the alloying ones.

Where the lot value justifies it, the check runs before the carton closes, while a replacement casting is still possible.

Four Blocks In A Casting Quote

Metal. Part weight in kilograms times the alloy price. This is the smallest block on a small part and the largest on a heavy one.

Tooling. One die, amortised across the order. The same die costs the same whether you order three thousand parts or thirty thousand, which is why the unit price falls so fast.

Cycle. Shots per hour, cavities per die, and the labour to trim and tumble the runners off.

Finish and rejects. Plating per square centimetre, painting per part, and the share that fails after plating.

Put numbers on it. If a die is quoted at 12,000 dollars and the order is 3,000 pieces, the die adds 4.00 dollars to every part.

At 30,000 pieces the same die adds 0.40. Nothing about the casting changed; only the number of parts sharing one tool.

That is why a second order is cheaper than the first. It is also why a supplier who will not separate the tooling line has something folded into the price.

Ask for tooling as a separate line. When a quote folds the die into the unit price, a reorder at a lower volume quietly becomes a different price.

Six Lines For The Order Sheet

One. Grade and standard: Zamak 3 to ASTM B86, or the European equivalent, or the Chinese one.

Two. Composition limits, written out. At minimum lead, cadmium and tin, because those decide whether the lot ages.

Three. Weight per piece, with a tolerance, and the wall thickness at the thinnest point.

Four. Finish: plating type, thickness in microns, colour, and the nickel release requirement if the part touches skin.

Five. The tests and the sample size, including the tape test and the drop height.

Six. Tooling ownership, and what happens to the die if the volume never repeats.

For the sourcing side of the same order, the jewellery sourcing walkthrough walks the process, and the smaller-part version shows the same checks on a smaller part.

GRADE AND PURITY

Send a casting drawing or a quotation. I will check the grade against the standard, the impurity caps and the wall at its thinnest point. The tooling line and the nickel report get the same look. No cost, no obligation.

Check My Drawing

Questions Buyers Ask

What is zamak made of?

Zinc with about 4 percent aluminium, a fraction of a percent of magnesium, and copper that varies by grade. Zamak 3 is roughly 96 percent zinc; grade 5 adds about 1 percent copper and grade 2 about 3.

Is zamak the same as pot metal?

No. Pot metal is a loose term for any cheap casting alloy, often made from scrap with no control on impurities. Zamak is the controlled version of the same idea, with named grades and capped lead, cadmium and tin.

Does zamak rust?

It contains no iron, so it does not rust. Zinc does corrode, though, and a bare casting will dull and spot. That is why almost every zamak part sold at retail carries plating, paint or a conversion coat.

Why do old zamak parts crack and crumble?

Zinc pest: intergranular corrosion started by lead, cadmium or tin above the limits. The alloy swells and splits along grain boundaries. It is a material batch problem, not a design problem, and it shows up years later.

How heavy is zamak?

Density runs about 6.6 to 6.8 grams per cubic centimetre depending on grade, so a part is heavy for its size compared with aluminium. Weight per piece is the fastest check that the die produced a full shot.

Is zamak jewellery safe to wear?

Zamak itself is used widely in costume jewellery. The skin contact question is about the finish. Nickel release must stay under 0.5 micrograms per square centimetre per week, and a plated part needs a report covering the plated surface.

Questions & Comments

We read every one and reply within 24 hours

If a casting drawing or a quotation crosses your desk, send it over. I will check the grade, the impurity caps and the wall at its thinnest point.

Subscribe
Notify of
guest
0 Comments
Most Voted
Newest Oldest
0
Would love your thoughts, please comment.x
()
x