Poly Mailer Manufacturer: The Edge Weld Fails
Home
Yiwu, Zhejiang, China
Mon – Fri 9:00 AM – 6:00 PM · Sat 9:00 AM – 4:00 PM
[email protected]

Poly Mailer Manufacturer: The Edge Weld Is the Product

Alan Xiao, Founder of Sourcing Pioneer
Alan Xiao Founder, Sourcing Pioneer
· Updated October 28, 2026 · 9 min read

A poly mailer is a bag that has to survive a conveyor belt, a sorting machine and a doorstep. It looks like a simple product, and the part that decides whether it arrives intact is the weld along the edge, not the film. The sheet that fixes the gauge, the weld and the tape is where a mailer order is decided.

Studio still life on a flat cream surface showing a white poly mailer with its adhesive strip open, a second mailer sealed with a printed surface, and a short strip of edge weld material, with a navy serif headline reading POLY MAILER and an amber subhead reading EDGE FIRST
Film, weld and tape. Two of the three are made on the machine.

The Short Answer

Four numbers decide a mailer: film gauge, weld width, adhesive type and print.

The film sets the strength. The weld sets whether the strength matters, because a bag that splits along the edge was never as strong as its film.

Ask for the gauge in microns and the weld width in millimetres. A supplier who answers both runs this product every day.

Flat vector diagram on a cream background with three labelled columns reading FILM, WELD and TAPE inside one outlined strip, with the note TWO ARE MADE ON THE LINE.
Three parts, two of them made on the machine.

What a Mailer Is Made Of

A mailer is film, two welds, an adhesive strip and a release liner.

The film is blown or cast, and most mailers use two or three layers co-extruded together. A black inner layer hides the contents. A white outer layer takes print.

The welds are made by heat and pressure, on the sides and across the bottom. The mouth carries the adhesive strip.

The liner covers the strip until it is used. A poor liner releases too early in a warm van, and the bag is unusable before it reaches a packer.

Film: Gauge, Layers and Opacity

Gauge is the thickness, written in microns. A thicker film resists a puncture and costs more to ship.

Layers matter more than buyers expect. A three-layer film can put a tough skin outside and a soft layer inside. That is why it bursts less than a single layer of the same total gauge.

Opacity is the privacy question. A thin white film shows a dark box through it, and that is the complaint that arrives with a photograph.

Ask for the gauge per layer, not only the total. A supplier who quotes a total without layers is describing a film, not a structure.

A co-extruded film is made in one pass, with the layers bonded while hot. A laminated film is glued in a second step. The first is cheaper and the second holds print better, which is why a heavy print job sometimes arrives on a laminated bag.

Ask which one is being quoted. Two bags that look the same in a sample differ in how they behave when a corner is dropped.

Ask too whether recycled content is in the mix, and what percentage. Recycled resin changes the colour and the strength, so a claim and a spec have to be written together.

The Weld: Width, Temperature and Speed

The weld is a strip where two layers of film are melted together. Its width is measured in millimetres.

A narrow weld is cheap and fails first. A wide weld takes more heat and more time on the machine, and it holds when a corner is pulled.

Temperature and speed are the other two settings. A line pushed fast runs a cooler weld, and a cool weld looks fine until a bag is filled.

Ask for the weld width and the peel strength. Peel strength is measured by pulling the two layers apart and recording the force.

A wide weld is not automatically better. A weld that is too wide stiffens the edge, and a stiff edge cracks when the bag flexes in a mail sack.

Ask how the weld behaves at the corner, where the side weld meets the bottom weld. That cross is the point most bags split.

The weld is made by a heated bar, and the film has to be clean for it to hold. A film with dust or too much slip additive seals weakly. That is why the same machine turns out good bags on Monday and weak ones on Friday.

Ask whether the film is corona treated before printing. The treatment raises the surface energy so ink and adhesive grip, and an untreated film looks fine until the print rubs off in a sorter.

A check that pulls a filled bag catches the batch where the machine ran hot and fast for an hour.

The Adhesive Strip and the Liner

The strip is what closes the bag. It is a coated band of adhesive with a liner over it.

Two things go wrong. The adhesive is too weak, and the bag opens in transit. The adhesive is too strong, and the customer cannot open it without a knife, which is worse for returns.

Ask for the adhesive type and the peel figure. A hot melt adhesive grips a rough surface; an acrylic one holds better in cold weather.

Ask how the strip behaves after two openings. Many customers open, check and reseal. A strip that seals once is a bag that cannot be returned in the same bag.

The liner matters in a warm warehouse. A liner that releases early leaves an exposed strip that sticks to the next bag in the stack.

Ask how the bags are packed for storage. A stack under pressure in a warm room will bond to itself. A bag that cannot be opened is a bag that is thrown away.

Ask for the shelf figure on the adhesive. A strip that holds for six months is different from one that holds for two years, and the price differs too.

The Tear Strip

A tear strip is a narrow band that opens the bag in one pull.

It is a convenience and a risk. A strip that is too easy to start opens in the sorting machine. A strip that is too hard is ignored, and the customer cuts the bag instead.

Ask whether the strip is printed with an instruction, and where it sits relative to the weld. A strip placed across a weld cannot be pulled cleanly.

A printed arrow costs almost nothing and cuts support questions. It is the cheapest upgrade in the whole order.

FilmWhat it givesWhere it fails
Single layerLowest price per bagPunctures at a corner
Two layerA white face and a dark innerSplits if the weld runs cold
Three layerA tough skin and a soft coreCosts more per micron
Recycled contentA claim you can printHazier, and weaker at the same gauge

Print on Film

Mailers are printed on a flexo press, usually in one or two colours.

Film stretches as it runs, so registration is looser than on paper. A design with a border will look wavy, and a solid block will look uneven at the edges.

Ask for the print tolerance and a printed sample, not a digital proof. A proof shows the artwork. A sample shows what the film does to it.

Ask which surface is printed. Print on the outside takes the scuffs of transit. Print on the inside shows through and cannot be scratched, but it limits the colours.

Ask how the ink is cured. A water based ink on a treated film is the usual answer. A solvent ink on the same film can block in a warm stack.

Four Tests Before the Batch

Burst, seal peel, adhesive and water. Four tests cover almost every failure this product has.

The burst test fills a bag with a weight and drops it onto a hard floor on a corner. A bag that splits at the weld was welded cold.

The test can be run in a back room. Fill three bags to your normal shipping weight, tape them shut and drop each one on a corner from waist height. Two splits out of three is a batch to reject.

The seal peel test pulls the edge apart and records the force. Two bags from the same batch should read close to the same figure.

The adhesive test closes a bag, opens it and closes it again. A strip that fails the second close costs a return.

The water test leaves a filled bag in the rain for an hour. Film keeps water out; a weld with a pinhole does not.

Test methods for plastic film are published by standards bodies, and the body that writes those methods names the procedure for each.

Nine Lines a Mailer Quote Needs

LineWhat it must state
SizeWidth by length, and the usable opening
FilmGauge per layer, and the resin
OpacityColour outside, and what shows through
WeldWidth in mm, and the peel figure
TapeAdhesive type, and the liner
Tear stripYes or no, and where it sits
PrintColours, surface, and tolerance
PackingBags per pack, and packs per carton
MinimumPer size, and per print run

The usable opening line is easy to miss. A bag measured outside loses a few millimetres to each weld, and a tight bag is slow to pack.

Minimums and the Plate

A plain mailer has one minimum: the machine run. A printed mailer has two, because the plate is charged before the first bag.

The plate is cheap compared with a cup or a bag, and it still sits on the first order. Ask whether it is charged once and whether it is stored.

Stock sizes are the way into the product. A stock width in a plain film needs no plate, and the only new cost is the print if there is one.

Ask what the minimum is per size in a mixed order. A supplier who runs several widths can take a mixed pallet that a single-line shop cannot.

Ask how the bags are counted. A pack of a hundred is a count, not a weight, and a short pack is invisible until a customer counts.

Where Mailers Are Made

Mailer production clusters near film extrusion, because a bag is a film tube welded and cut.

So a supplier may blow the film and weld it, or buy film and weld it. Ask which one, because the second supplier can change film without telling you.

Ask how many extruders run and what the smallest run is. A supplier with one line turns down a small order and a supplier with three may not.

The clause that keeps the plate and the film spec on file is worth a sentence, because a film change is invisible in a sample.

Freight and the Last Cost

Mailers are light and bulky, and they ship flat in packs.

Ask for bags per pack, packs per carton, and the carton dimensions. Then compare the volume against the price.

How a forwarder bills a flat carton is the last line in the sum, and a cheap bag in a big carton is not cheap.

The drop routine a packed carton must pass matters here too, because cartons of mailers are often stacked high in a container.

Recyclability and the Claim

Most mailers are made of a low density film, which is collected in some places and not in others.

A recyclability claim has to match the collection system where the customer lives. A bag that is recyclable in theory and not collected in practice is a claim that invites a complaint.

Ask for the resin code and the recycled content. Check what your market accepts before printing anything on the bag.

Some markets now charge a producer for the packaging they put on the market. That fee lands on the brand, not the supplier, and a lighter bag lowers it.

So a gauge decision is also a fee decision. Ask what the bag weighs and multiply it across the year before choosing the heaviest film.

On the import side, a plain mailer and a printed mailer can sit in different places in the tariff schedule. The printed article has a different identity from the film it started as. The tariff database published by the commission is where the line is fixed.

Questions Buyers Ask About Poly Mailer Suppliers

Why do my mailers split at the corner?

The weld runs cold at the cross where the side meets the bottom. Ask for a wider weld and a peel figure.

What gauge should I use?

Heavy enough for the weight and the route. Ask for layers as well as total gauge, because structure beats thickness.

Can customers see what is inside?

With a thin white film, sometimes. A black inner layer is the usual fix.

Is a tear strip worth it?

For returns and for a clean opening, yes. For heavy goods it can start a tear that ruins the bag.

Are poly mailers recyclable?

They can be, where the film is collected. The claim has to match the local system.

Do I pay a plate for print?

Once, if it is kept. Ask before the first order, not after.

The Bottom Line

Price the film, the weld and the tape as three decisions, then fill a bag and drop it on a corner. The weld is where the money goes when a package arrives open.

A bag that holds its seal and hides its contents is worth more than a micron saved. The micron is invisible and the split is not.

EDGE FIRST

Send the Size

Send the size, the weight you will ship and the print you want. We will price two gauges and two weld widths, drop a filled bag on a corner to see where it splits, and show what the carton adds to the landed cost.

Send the Size

Questions & Comments

We read every one and reply within 24 hours

Had a package arrive split along the edge, or a tape that let go in the van? Send the gauge and the weld width. We will say which of the two was never measured.